Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (24): 537-542    DOI:
Current Issue | Archive | Adv Search |
COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT
CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology)
Cite this article: 

CAO Zhenning(Shandong Polytechnic Unversity; Jinan);WU Chuansong; WU Lin (Harbin Institute of Technology). COMPUTER SIMULATION OF MIG WELD POOLS WITH DROPLET IMPACT. Acta Metall Sin, 1994, 30(24): 537-542.

Download:  PDF(426KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Combined behaviour of droplets with pools in MIG welding, a numerical analysis model has been developed for three-dimensional fluid flow and heat transfer in MIG weld pools with droplet impact. Droplet heat energy and momentum carried off into pool as well as pool-surfaee deformation were fully considered. Fluid flow field, temperature distribution and pool-surface deformation are successfully simulated.
Key words:  computer simulation      MIG weld pool      droplet impact     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I24/537

1PadoE,WeckamnDC.MetallTrans,1989;20B:9372TsaoKC,WuCS.WeldJ,1988;67:70-s3武传松,吴林,陈定华.焊接学报,1991;12:1894ChooRTC,MukaiK,ToguriJM.WeldJ,1992;71:139-s5EssersWG,WalterR.WesdJ,1981;60:37-s6武传松,曹振宁,吴林.金属学报,1992;28:B4277KouS,WangYH.WeldJ1986;65:63-s8WoodsRA.WeldJ,1971;50:163-s9HeipleCR,RoperJR.Weld,1982;61:97-s
[1] ;. STUDY OF 3D QUASI--STATIONARY GRAIN SIZE DISTRIBUTION DERIVED FROM MACPHERSON—SROLOVITZ TOPOLOGY--RELATED GRAIN GROWTH RATE EQUATION[J]. 金属学报, 2008, 44(7): 769-774 .
[2] zhang lin. Modelling structural changes of a molten Cu55 cluster on cooling by molecular dynamics[J]. 金属学报, 2008, 44(10): 1161-1166 .
[3] HOU Hua; ZHAO Yuhong; CHEN Zheng; XU Hong. Prediction for the Early Precipitation Process of Ni75AlxV25-X System with Lower Al Concentration by the Phase-Field Model[J]. 金属学报, 2005, 41(7): 695-702 .
[4] ZHANG Lin; ZHANG Caibei; WANG Yuanming; WANG Shaoqing. Cellular Automaton Modelling Of The Transformation From Austenite to Ferrite In Low Carbon Steels During Continuous Cooling[J]. 金属学报, 2004, 40(1): 8-13 .
[5] CHU Yelong; XIONG Liangyue; SUN Xiaokai (Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). COMPUTER STUDY OF MAGNETIZATION IN NANOCOMPOSITE MAGNETS[J]. 金属学报, 1998, 34(4): 423-430.
[6] SUI Zhitong;ZHANG Peixin(Northeastern University; Shenyang 110006). SELECTIVE PRECIPITATING BEHAVIOR OF THE BORON COMPONENTS FROM THE BORON SLAGS[J]. 金属学报, 1997, 33(9): 943-951.
[7] WU Chuansong (Shandong University of Technology; Jinan 250061); L. DORN (Berlin Technical University; Germany). THE INFLUENCE OF DROPLET IMPACT ON METAL INERT GAS WELD POOL GEOMETRY[J]. 金属学报, 1997, 33(7): 774-780.
[8] YIN Aijun; LI Jing; LI Hinhai; HUANG Kexiong; JIANG Hanying (Central South University of Technology; Changsha 410083) (Manuscript received 1995-06-30; in revised form 1995-12-01). COMPUTER SIMULATION ON MINOR ELEMENT BEHAVIOUR IN COPPER FLASH SMELTING[J]. 金属学报, 1996, 32(4): 387-392.
[9] CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18). SIMULATION OF INDENTATION MICROHARDNESS TESTING[J]. 金属学报, 1995, 31(13): 44-5.
[10] CHEN Da;LU Min;LIN Dongliang (Lin T L) Shanghai Jiao Tong UniversityDepartment of Materials Science;Shanghai Jiao Tong University; Shanghai 200030. SIMULATIVE STUDY OF INTERACTION BETWEEN GRAIN BOUNDARIES AND DISLOCATIONS IN Ni_3Al[J]. 金属学报, 1993, 29(7): 34-39.
[11] SHAO Jun;XU Hua;CHENG Ailan;KLEIN M. L. University of Pennsylvania; Philadelphia; U. S. A; State University of New York; U. S. A.; University of Pennsylvania; Philadelphia; U. S. A.. CONSTANT PRESSURE MOLECULAR DYNAMICS SIMULATION OF MOLTEN LiF-BeF_2 SYSTEM[J]. 金属学报, 1993, 29(1): 59-64.
[12] YAN Wen Xi'an Institute of Technology Correspondent associate professor;xi'an Institute of Technology. SYMMETRICAL SUPERLATTICE INTRINSJC STACKING FAULTS IN DEFORMEDPOLYCRYSTALLINE Ni_3 Al AND THEIR FORMATION MECHANISM[J]. 金属学报, 1991, 27(5): 8-13.
[13] WANG Xi;ZHOU Jiankun;CHEN Youshan;LIU Xianghuai;ZOU Shichang Ion Beam Laboratory; Shanghai Institute of Metallurgy; Academia Sinica. COMPUTER SIMULATION OF ION BEAM ENHANCED DEPOSITION OF TiN FILMS[J]. 金属学报, 1991, 27(3): 136-141.
[14] WEI Chao;QIAN Rengen;LIN Shi;XIAO Jimei University of Science and Technology Beijing Department of mathematics and mechanics; University of Science and Technology Beijing; Beijing 100083. COMPUTER SIMULATION OF EFFECT OF ORIENTATION DIFFERENCE ON MECHANICAL PROPERTIES OF BICRYSTALLINE SPECIMENS[J]. 金属学报, 1990, 26(4): 18-21.
[15] LIN Dongliang;CHEN Da T. L. Lin Shanghai Jiaotong University professor;Department of Materials Science;Shanghai Jiaotong University;Shanghai 200030. COMPUTER SIMULATION OF GRAIN BOUNDARY STRUCTURES IN Ni_3 Al[J]. 金属学报, 1990, 26(3): 10-17.
No Suggested Reading articles found!