| ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS |
| CHE Hiaozhou; HU Gengxiang(Shanghai Jiaotong University); CAO Hingguo(Luoyang Institute of Technology); DAI Lizhi(Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing) |
|
Cite this article:
CHE Hiaozhou; HU Gengxiang(Shanghai Jiaotong University); CAO Hingguo(Luoyang Institute of Technology); DAI Lizhi(Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing). ANNEALING EMBRITTLEMENT OF AMORPHOUS Fe-B-Si ALLOYS. Acta Metall Sin, 1994, 30(24): 532-536.
|
|
|
Abstract Annealing embrittlement of the amorphous Fe-B-Si alloys is strongly dependent on their composition and is relatively susceptible to melt-quenching condition and annealing treatment. Alloys composed near the eutectic range, such as amorphous Fe80B11.5Si8.5 and Fe79B11.5Si9.5 alloys, and the ultra-thin ribbons made from suitable melt-spun technique are slightly tending to annealing embrittlement. Compared to conventional annealing regime,rapid annealing by pulse-current heating can obviously improve the magnetic properties of as-quenched alloys with holding the ductility. It is a hopeful practical method to obtain an optimum ductile and superior magnetic properties of amorphous Fe-B-Si alloy.
|
|
|
| 1张传历.国外金属材料,1982;11:392LuborskyFE,WalterJL,JApplPhys,1976;47:36483车晓舟,曹兴国,戴礼智.机械工程材料,1993;17(4):174YamasakiT,TakahashiM,OginoY,In:SteebS,WarlimontHeds.,RapidlyQuenchedMetals,Vol.II,ElsevierSciencePublishersB.V.,1984:13815WangJT,PangDX,SongQH,DingBZ.MaterSciEng,1988;98:5356ChiGC,ChenHS,MillerCE.JApplPhys,1978;49:1715f |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|