Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (23): 477-483    DOI:
Current Issue | Archive | Adv Search |
IN SITU TEM OBSERVATION OF DISLOCATION EMISSION,MOTION AND SCC INITIATION IN Ti_3Al+Nb UNDER METHANOL CORROSION
GAO Kewei;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1995-02-27)
Cite this article: 

GAO Kewei;CHU Wuyang;XIAO Jimei(University of Science and Technology Beijing;Beijing 100083)(Manuscript received 1995-02-27). IN SITU TEM OBSERVATION OF DISLOCATION EMISSION,MOTION AND SCC INITIATION IN Ti_3Al+Nb UNDER METHANOL CORROSION. Acta Metall Sin, 1995, 31(23): 477-483.

Download:  PDF(629KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The in situ TEM observations of dislocation emission,motion and initiation of nanocrack in Ti_3Al+Nb under methanol corrosion were carried out.Using a special constant displacement device,the dislocation coniguration change ahead of a loaded crack tip before and after anodic dissolution in methanol and the initiation,propagation of nanometre scale stress corrosion cracks have been observed.The results showed that localized anodic dissolution of Ti_3Al+Nb in methanol at room temperature facilitated dislocation emission,multiplication and motion.A nanocrack initiated in the dislocation free zone or at the blunted crack tip after dislocation emission, multiplication and motion reached a critical condition.
Key words:  Ti_3Al+Nb      dislocation emission      stress corrosion crack      TEM in situ observation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I23/477

1UhligHH.JElectrochemSoc,1976;123:16992RevieRW,UhligHH.ActaMetall,1974;22:6193SmialowskiM,KostanskingJ.CorrosSci,1979;19:10194Gu8,ChuWY,QiaoLJ,HsiaoCM,ScrMetallMater,1994;31:1615黄彦良,曹楚南,林海潮.金属学报,1993,29:B2126魏学军,周向阳,柯伟,金属学报,1993;29:B2697KanfmanMJ,FinkJI.ActaMetal,1985;36:22138褚武扬.氢损伤与滞后断裂.北京:冶金工业出版社,1988:3619张跃,褚武扬,王燕斌.乔利杰,肖纪美.金属学报,1994;30:A3510MagninT,ChieragattiR,OltraR.ActaMetallMater,1990;38:13l311JonesDAMetallTrans,1985;16A:113312黄一中,陈奇志,袁昌言,褚武扬.金属学报,1994;30:B45313RiceJR,ThomsonR.PhilosMag,1974,29:7314陈奇志,褚武扬,肖纪美,中国科学,1994;A24:115高克玮,陈奇志,褚武扬,肖纪美.中国科学,1994,A24:99316张跃,褚武扬,王燕斌,肖纪美.中国科学,1994,A24.55117OhrSM.MaterSciEng,1985;72:118谷飘,张静武,万发荣,褚武扬.金属学报,1995,31:A15619ZhangY,WangYB,ChuWY,HsiaoCM.ScrMetallMater,1992;26:926
[1] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[2] MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei. Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy[J]. 金属学报, 2022, 58(9): 1118-1128.
[3] Hongchi MA, Cuiwei DU, Zhiyong LIU, Yong LI, Xiaogang LI. Comparative Study of Stress Corrosion Cracking Behaviors of Typical Microstructures of Weld Heat-Affected Zones of E690 High-Strength Low-Alloy Steel in SO2-Containing Marine Environment[J]. 金属学报, 2019, 55(4): 469-479.
[4] Ping DENG,Chen SUN,Qunjia PENG,En-Hou HAN,Wei KE,Zhijie JIAO. Study on Irradiation Assisted Stress Corrosion Cracking of Nuclear Grade 304 Stainless Steel[J]. 金属学报, 2019, 55(3): 349-361.
[5] Jun YU, Deping ZHANG, Ruosheng PAN, Zehua DONG. Electrochemical Noise of Stress Corrosion Cracking of P110 Tubing Steel in Sulphur-Containing Downhole Annular Fluid[J]. 金属学报, 2018, 54(10): 1399-1407.
[6] Hongzhong YUAN,Zhiyong LIU,Xiaogang LI,Cuiwei DU. Influence of Applied Potential on the Stress Corrosion Behavior of X90 Pipeline Steel and Its Weld Joint in Simulated Solution of Near Neutral Soil Environment[J]. 金属学报, 2017, 53(7): 797-807.
[7] Shu GUO,En-Hou HAN,Haitao WANG,Zhiming ZHANG,Jianqiu WANG. Life Prediction for Stress Corrosion Behavior of 316L Stainless Steel Elbow of Nuclear Power Plant[J]. 金属学报, 2017, 53(4): 455-464.
[8] Hongliang MING,Zhiming ZHANG,Jianqiu WANG,En-Hou HAN,Mingxing SU. Microstructure and Local Properties of a Domestic Safe-End Dissimilar Metal Weld Joint by Using Hot-Wire GTAW[J]. 金属学报, 2017, 53(1): 57-69.
[9] Maocheng YAN,Shuang YANG,Jin XU,Cheng SUN,Tangqing WU,Changkun YU,Wei KE. STRESS CORROSION CRACKING OF X80 PIPELINE STEEL AT COATING DEFECT IN ACIDIC SOIL[J]. 金属学报, 2016, 52(9): 1133-1141.
[10] Zhiyong LIU,Zongshu LI,Xiaolin ZHAN,Wenzhu HUANGFU,Cuiwei DU,Xiaogang LI. GROWTH BEHAVIOR AND MECHANISM OF STRESS CORROSION CRACKS OF X80 PIPELINE STEEL IN SIMULATED YINGTAN SOIL SOLUTION[J]. 金属学报, 2016, 52(8): 965-972.
[11] Zilong ZHANG, Shuang XIA, Wei CAO, Hui LI, Bangxin ZHOU, Qin BAI. EFFECTS OF GRAIN BOUNDARY CHARACTER ON INTERGRANULAR STRESS CORROSION CRACKING INITIATION IN 316 STAINLESS STEEL[J]. 金属学报, 2016, 52(3): 313-319.
[12] Hongchi MA, Cuiwei DU, Zhiyong LIU, Wenkui HAO, Xiaogang LI, Chao LIU. STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE[J]. 金属学报, 2016, 52(3): 331-340.
[13] Ju KANG,Jichao LI,Zhicao FENG,Guisheng ZOU,Guoqing WANG,Aiping WU. INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY[J]. 金属学报, 2016, 52(1): 60-70.
[14] Yueling GUO, En-Hou HAN, Jianqiu WANG. EFFECTS OF FORGING AND HEAT TREATMENTS ON STRESS CORROSION BEHAVIOR OF 316LN STAINLESS STEEL IN HIGH TEMPERATURE CAUSTIC SOLUTION[J]. 金属学报, 2015, 51(6): 659-667.
[15] YAN Maocheng, WANG Jianqiu, HAN En-hou, SUN Cheng, KE Wei. CHARACTERISTICS AND EVOLUTION OF THIN LAYER ELECTROLYTE ON PIPELINE STEEL UNDER CATHODIC PROTECTION SHIELDING DISBONDED COATING[J]. 金属学报, 2014, 50(9): 1137-1145.
No Suggested Reading articles found!