Abstract The partial α(α_2)/γ phase equilibria in Ti-Al-Ga and Ti-Al-Nb-Cr systems at lower Ga,Nb and Cr were measured by EPMA.Composition distribution ratio equations of Ga,Nb,Cr in α(α_2)/γ equilibria phases were deduced and γ phase stabilization parameters of Ga,Nb,Cr at various temperatures were calculated by using equations.The results show that Ga and Nb are γ phase-forming elements,while Cr isαphase-forming element.