LI Jianmin;SUN Wensheng;QUAN Mingxiu; HU Zhuangqi(State Key Laboratory for RSA;Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015);WANG Yongzhong;QIAO Guiwen(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1994-05-04;in revised form 1995-03-28)
Cite this article:
LI Jianmin;SUN Wensheng;QUAN Mingxiu; HU Zhuangqi(State Key Laboratory for RSA;Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015);WANG Yongzhong;QIAO Guiwen(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1994-05-04;in revised form 1995-03-28). DUCTILE-BRITTLE TRANSITION OF(Fe_0.99)Mo_(0.01))_(78)Si_9B_(13) AMORPHOUS ALLOY. Acta Metall Sin, 1995, 31(23): 493-498.
Abstract Ductile-brittle (D-B) transition of(Fe_0.99Mo_0.01)_78Si_9B_13 amorphous ribbon annealed at 244℃ was investigated.D-B transition is associated with the precipitation of nanometer-sized polycrystallite α-Fe(Si,Mo) from amorphous matrix and void formation.