Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (23): 493-498    DOI:
Current Issue | Archive | Adv Search |
DUCTILE-BRITTLE TRANSITION OF(Fe_0.99)Mo_(0.01))_(78)Si_9B_(13) AMORPHOUS ALLOY
LI Jianmin;SUN Wensheng;QUAN Mingxiu; HU Zhuangqi(State Key Laboratory for RSA;Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015);WANG Yongzhong;QIAO Guiwen(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1994-05-04;in revised form 1995-03-28)
Cite this article: 

LI Jianmin;SUN Wensheng;QUAN Mingxiu; HU Zhuangqi(State Key Laboratory for RSA;Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015);WANG Yongzhong;QIAO Guiwen(Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015) (Manuscript received 1994-05-04;in revised form 1995-03-28). DUCTILE-BRITTLE TRANSITION OF(Fe_0.99)Mo_(0.01))_(78)Si_9B_(13) AMORPHOUS ALLOY. Acta Metall Sin, 1995, 31(23): 493-498.

Download:  PDF(420KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Ductile-brittle (D-B) transition of(Fe_0.99Mo_0.01)_78Si_9B_13 amorphous ribbon annealed at 244℃ was investigated.D-B transition is associated with the precipitation of nanometer-sized polycrystallite α-Fe(Si,Mo) from amorphous matrix and void formation.
Key words:  Fe-based amorphous alloy      anneal-embrittle      free volume     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I23/493

1LuborskyFE.JApplPhys,1976;47:36482SpaepenF.ActaMetall,1977;25:4073FreedRL,VanderSandeJB,ActaMetall,1980;28:1034 王隆保.金属学报,1992:28:B625KomatsuDM.JNon-CrystSolid,1987;91:526 KomatsuT.JNon-CrystSolids,1987;91:527NoldE,LamparterP,OlbrichH,Rainer-HarbachA,SteebS.ZNaturforsch,1981;36a:10328ArgonAS.ActaMetall,1979;27:47
[1] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[2] HU Qiang ZENG Xierong QIAN Haixia XIE Shenghui SHENG Hongchao. CORRELATION BETWEEN THE GLASS-FORMING ABILITY AND CHARACTERISTIC FREE VOLUMES OF THE IRON BASE BULK METALLIC GLASSES[J]. 金属学报, 2012, 48(11): 1329-1334.
[3] XU Min YI Jun QUAN Mingxiu WANG Yandong ZUO Liang. EFFECT OF Nb ON CRYSTALLIZATION KINETICS OF Fe-Co-Nd-B AMORPHOUS ALLOYS[J]. 金属学报, 2009, 45(1): 91-96.
[4] QIAN Xiangrong;ZHOU Yicang;ZHANG Dongbin;MA Ruzhang Shanghai Iron and Steel Research Institute; Y. T. Chou Lehigh University; U. S. A.; University of Science and Technology Beijing. CORRELATION BETWEEN GRAIN BOUNDARY CORROSION AND MISORIENTATION IN Nb BICRYSTALS[J]. 金属学报, 1993, 29(2): 83-87.
[5] YANG Huisheng; XIONG Xiaotao; XU Zuxiong; MA Ruzhang (University of Science and Technology Beijing); TU Guochao; ZHANG Jiaji (Institute of Metallurgy; Shoudu Iron and Steel Company). X-RAY DIFFRACTION STUDY ON CRYSTALLIZATION OF AMORPHOUS Fe (76.5)Cu_1Si_(13.5)B_9 ALLOY[J]. 金属学报, 1992, 28(11): 75-80.
No Suggested Reading articles found!