Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (23): 523-526    DOI:
Current Issue | Archive | Adv Search |
EUTECTIC CARBIDE GRANULATION OF CAST Cr12 DIE STEEL
WANG Shuqi;JIANG Qichuan;ZHAO Yuguang;HE Zhenming(Jilin University of Technology;Changchun 130025)(Manuscript received 1994-11-11;in revised form 1995-07-26)
Cite this article: 

WANG Shuqi;JIANG Qichuan;ZHAO Yuguang;HE Zhenming(Jilin University of Technology;Changchun 130025)(Manuscript received 1994-11-11;in revised form 1995-07-26). EUTECTIC CARBIDE GRANULATION OF CAST Cr12 DIE STEEL. Acta Metall Sin, 1995, 31(23): 523-526.

Download:  PDF(321KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By means of the modification of multiple compound agent,eutectic structure of cast Cr12 die steel is refined and the amount of divorced eutectic is increased.After heat treatment,network eutectic carbides of cast Cr12 die steel are changed into granular and dispersed ones.The impact toughness is greatly increased.It ensures the application of cast Cr12 die steel.
Key words:  Cr12 steel      cast die      modification      eutectic carbide granulation     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I23/523

1郭建亭,周福振.机械工程学报,1981;17(2):282佐藤敬.铸物,1972:44(2):7983DiesbergD,E.Giesserei.1976;63(2):254MaNaiheng,RaoQichang,ZhouQingde.TransAmFoundrymen'sSoc,1990;98:7755王兆昌.北京钢铁学院学报,1986;8(2):226姜启川,阎久林,关庆丰,王守实,荣福杰,李章.金属学报,1992;28:B4597王兆昌,马前.铸造,1989;(11):18毛卫民,钟雪友.金属学报,1993;29:A4929张景辉,李大军,潘金虎,贾均,叶荣茂,李剑慧.铸造.1989;(11):7
[1] LIU Lujun, LIU Zheng, LIU Renhui, LIU Yong. Grain Boundary Structure and Coercivity Enhancement of Nd90Al10 Alloy Modified NdFeB Permanent Magnets by GBD Process[J]. 金属学报, 2023, 59(11): 1457-1465.
[2] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[3] GAO Han, LIU Li, ZHOU Xiaoyu, ZHOU Xinyi, CAI Wenjun, ZHOU Hongling. Preparation and Bioactivity of Micro-Nano Structure on Ti6Al4V Surface[J]. 金属学报, 2023, 59(11): 1466-1474.
[4] CUI Zhenduo, ZHU Jiamin, JIANG Hui, WU Shuilin, ZHU Shengli. Research Progress of the Surface Modification of Titanium and Titanium Alloys for Biomedical Application[J]. 金属学报, 2022, 58(7): 837-856.
[5] YANG Lipo, ZHANG Hailong, ZHANG Yongshun. Present Analysis and Trend Prediction of Shape/ Performance Collaborative Control for High-End Cold Rolling Foils[J]. 金属学报, 2021, 57(3): 295-308.
[6] Di ZHANG, Mengying YUAN, Zhanqiu TAN, Ding-Bang XIONG, Zhiqiang LI. Progress in Interface Modification and Nanoscale Study of Diamond/Cu Composites[J]. 金属学报, 2018, 54(11): 1586-1596.
[7] Erlin ZHANG, Xiaoyan WANG, Yong HAN. Research Status of Biomedical Porous Ti and Its Alloy in China[J]. 金属学报, 2017, 53(12): 1555-1567.
[8] Xiao LIN, Jun GE, Shuilin WU, Baohua LIU, Huilin YANG, Lei YANG. Advances in Metallic Biomaterials with both Osteogenic and Anti-Infection Properties[J]. 金属学报, 2017, 53(10): 1284-1302.
[9] Zhentao YU, Sen YU, Jun CHENG, Xiqun MA. Development and Application of Novel Biomedical Titanium Alloy Materials[J]. 金属学报, 2017, 53(10): 1238-1264.
[10] LUO Xinmin, WANG Xiang, CHEN Kangmin, LU Jinzhong, WANG Lan, ZHANG Yongkang. SURFACE LAYER HIGH-ENTROPY STRUCTURE AND ANTI-CORROSION PERFORMANCE OF AERO-ALUMINUM ALLOY INDUCED BY LASER SHOCK PROCESSING[J]. 金属学报, 2015, 51(1): 57-66.
[11] LUO Xinmin, CHEN Kangmin, ZHANG Jingwen, LU Jinzhong,REN Xudong,LUO Kaiyu, ZHANG Yongkang. DISLOCATION MECHANISM OF SURFACE MODIFICATION FOR COMMERCIAL PURITY ALUMINUM  AND ALUMINUM ALLOY BY LASER SHOCK PROCESSING[J]. 金属学报, 2013, 49(6): 667-674.
[12] YANG Lingxiao, GUO Xiping, QIAO Yanqiang, PAN Ruobing. FORMATION OF Ge-Y MODIFIED SILICIDE COATINGS ON Nb-Ti-Si BASE ULTRAHIGH TEMPERATURE ALLOY[J]. 金属学报, 2013, 49(11): 1433-1438.
[13] ZHAO Shengsheng CHENG Yu CHANG Zhengkai WANG Tiegang SUN Chao. MODIFICATION OF STRESS DISTRIBUTION ALONG THE THICKNESS OF (Ti, Al)N COATINGS AND PREPARATION OF THE COATINGS WITH LARGE THICKNESS[J]. 金属学报, 2012, 48(3): 277-282.
[14] ZHANG Fenggang ZHU Xiaopeng WANG Mingyang LEI Mingkai. SURFACE MODIFICATION OF WC-Ni CEMENTED CARBIDE FOR SEALS BY HIGH-INTENSITY PULSED ION BEAM IRRADIATION[J]. 金属学报, 2011, 47(7): 958-964.
[15] XIE Xishan DONG Jianxin FU Shuhong ZHANG Maicang. RESEARCH AND DEVELOPMENT OF γ´´ AND γ´ STRENGTHENED Ni-Fe BASE SUPERALLOY GH4169[J]. 金属学报, 2010, 46(11): 1289-1302.
No Suggested Reading articles found!