| EUTECTIC CARBIDE GRANULATION OF CAST Cr12 DIE STEEL |
| WANG Shuqi;JIANG Qichuan;ZHAO Yuguang;HE Zhenming(Jilin University of Technology;Changchun 130025)(Manuscript received 1994-11-11;in revised form 1995-07-26) |
|
Cite this article:
WANG Shuqi;JIANG Qichuan;ZHAO Yuguang;HE Zhenming(Jilin University of Technology;Changchun 130025)(Manuscript received 1994-11-11;in revised form 1995-07-26). EUTECTIC CARBIDE GRANULATION OF CAST Cr12 DIE STEEL. Acta Metall Sin, 1995, 31(23): 523-526.
|
|
|
Abstract By means of the modification of multiple compound agent,eutectic structure of cast Cr12 die steel is refined and the amount of divorced eutectic is increased.After heat treatment,network eutectic carbides of cast Cr12 die steel are changed into granular and dispersed ones.The impact toughness is greatly increased.It ensures the application of cast Cr12 die steel.
|
|
|
| 1郭建亭,周福振.机械工程学报,1981;17(2):282佐藤敬.铸物,1972:44(2):7983DiesbergD,E.Giesserei.1976;63(2):254MaNaiheng,RaoQichang,ZhouQingde.TransAmFoundrymen'sSoc,1990;98:7755王兆昌.北京钢铁学院学报,1986;8(2):226姜启川,阎久林,关庆丰,王守实,荣福杰,李章.金属学报,1992;28:B4597王兆昌,马前.铸造,1989;(11):18毛卫民,钟雪友.金属学报,1993;29:A4929张景辉,李大军,潘金虎,贾均,叶荣茂,李剑慧.铸造.1989;(11):7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|