Study on the Precipitation of γ' in a Fe-Ni Base Alloy During Ageing by APT
Yuanyuan SONG, Mingjiu ZHAO, Lijian RONG()
CAS Key Laboratory of Nuclear Materials and Safety Assessment, Institue of Metal Research, Chinese Academy of Sciences, Shenyang 110016, China
Cite this article:
Yuanyuan SONG, Mingjiu ZHAO, Lijian RONG. Study on the Precipitation of γ' in a Fe-Ni Base Alloy During Ageing by APT. Acta Metall Sin, 2018, 54(9): 1236-1244.
High strength Fe-Ni base austenitic alloys, such as A286 and JBK-75, are widely used in gas turbine jet engines and hydrogen service and so on because of their excellent corrosion resistance and low hydrogen embrittlement sensitivity. The ordered coherent γ' [Ni3(Al,Ti)], precipitated during ageing, is thought to have the main contribution on the strength. Thus, it is very important to understand the characterization of the precipitation. However, few previous studies are focused on atomic scale evolution of the precipitated phase. Atom probe tomography (APT) is a unique microscopy technique that provides 3D analytical mapping of materials at near atomic resolution and a high detection sensitivity for all elements. The present research is focused on the microstructure evolution at ageing temperature at different time scales using APT. A Fe-Ni base austenite alloy were aged at 620 ℃ for different time after solution treated at 980 ℃ for 2 h. Hardness testing indicates that a sharp increase is observed when the ageing time is less than 6 h. The hardness is up to 205 HV from the initial 145 HV at the ageing time 6 h. After that the hardness increases slowly. The hardness is 251 HV at 120 h. APT results reveal that Ti-rich nanoclusters precipitate obviously at the initial stage of ageing, which contain Fe, Cr, Ni, Mo and Al elements. As the ageing time increases, more Ni and Al atoms are segregated in the Ti-rich nanoclusters while the Fe, Cr and Mo are ejected from the nanoclusters. When the ageing time is up to 120 h, the Ni/(Ti+Al) ration is approximately close to 3. The precipitates can be identified as γ' phase. The results reveal that the formation of γ' involves nucleation and growth. Effect of the number density and the size of the γ' precipitates on the hardening of the alloy has been estimated.
Fig.1 Variation of Vickers hardness in the J75 steel solution treated at 980 ℃ for 1 h with ageing time at 620 ℃
Fig.2 Atom distribution maps of Fe, Cr, Mo, Ni, Ti and Al in J75 alloy solution treated at 980 ℃ for 1 h (a) and the nearest-neighbor count distributions of Al and Ti (b) (d-pair—distance between two atoms)
Fig.3 Atom distribution maps of Fe, Cr, Mo, Ni, Ti and Al in J75 alloy aged at 620 ℃ for 1 h (a) and the nearest-neighbour count distributions of Al and Ti (b), the clusters distribution (c) and distribution of Fe, Ni, Cr, Ti and Al atoms in analyzed volume of 20 nm×20 nm×2 nm (d) (The red cycles indicate the nanoclusters)
Fig.4 Atom distribution maps of Fe, Cr, Mo, Ni, Ti and Al in J75 alloy aged at 620 ℃ for 6 h (a) and the nearest-neighbor count distributions of Al and Ti (b), distribution of Fe, Ni, Cr, Ti , Al and Mo atoms in analyzed volume of 20 nm×20 nm×2 nm (Red cycles indicate the nanoclusters) (c) and one dimensional concentration profile along the arrow marked in Fig.4c (d)
Fig.5 Atom distribution maps of Fe, Cr, Mo, Ni, Ti and Al in J75 alloy aged at 620 ℃ for 16 h (a), the distribution of Fe, Ni, Cr, Ti, Mo and Al atoms in analyzed volume of 20 nm×20 nm×2 nm (Red cycles indicate the nanoclusters) (b) and one dimensional concentration profile along the arrow marked in Fig.5b (c)
Fig.6 Atom distribution maps of Fe, Cr, Mo, Ni, Ti and Al atoms in J75 alloy aged at 620 ℃ for 120 h
Fig.7 Isoconcentration surface of 11%(Al+Ti) (atomic fraction) in J75 alloy aged at 620 ℃ for 120 h (a) and one dimensional concentration profile (b), and the distributions of Fe, Ni, Cr, Ti, Mo and Al in analyzed volume of 10 nm× 10 nm× 2 nm (c)
Fig.8 Number density and volume fraction of nanoclusters or precipitates in J75 alloy aged at different time
[1]
Brooks J A, Thompson A W.Microstructure and hydrogen effects on fracture in the alloy A-286[J]. Metall. Trans., 1993, 24A: 1983
[2]
Li X Y, Li Y Y.The Hydrogen Damage of Austenite Alloys [M]. Beijing: Science Press, 2003: 1(李秀艳, 李依依. 奥氏体合金的氢损伤 [M]. 北京: 科学出版社, 2003: 1)
[3]
De Cicco H, Luppo M I, Gribaudo L M, et al.Microstructural development and creep behavior in A286 superalloy[J]. Mater. Character., 2004, 52: 85
[4]
Ma L M, Liang G J, Fan C G, et al.Effect of microstructure on hydrogen damage of JBK-75 precipitate-strengthened austenitic steel[J]. Acta. Metall. Sin.(Engl. Lett.), 1997, 10: 206
[5]
Guo J T.Materials Science and Engineering for Superalloys (Volume one)—Application of basic theory [M]. Beijing: Science Press, 2008: 300(郭建亭. 高温合金材料学(上册)-应用基础理论 [M]. 北京: 科学出版社, 2008: 300)
[6]
Rho B S, Nam S W.Fatigue-induced precipitates at grain boundary of Nb-A286 alloy in high temperature low cycle fatigue[J]. Mater. Sci. Eng., 2000, A291: 54
[7]
Li X Y, Zhang J, Rong L J, et al.Cellular η phase precipitation and its effect on the tensile properties in an Fe-Ni-Cr alloy[J]. Mater. Sci. Eng., 2008, A488: 547
[8]
Chen S H, Zhao M J, Rong L J.Role of γ' characteristic on the hydrogen embrittlement susceptibility of Fe-Ni-Cr alloys[J]. Corros. Sci., 2015, 101: 75
[9]
Birnbaum H K, Sofronis P.Hydrogen-enchanced localized plasticity—A mechanism for hydrogen-related fracture[J]. Mater. Sci. Eng., 1994, A196: 191
[10]
Guo Z F, Zhao M J, Li C F, et al.Mechanism of hydrogen embrittlement in a gamma-prime phase strengthened Fe-Ni based austenitic alloy[J]. Mater. Sci. Eng., 2012, A555: 77
[11]
Li Z W, Zhao M J, Rong L J.Study on behaviors of hydrogen-induced fracture of precipitation strengthened austenitic alloy[J]. Chin. J. Mater. Res., 2012, 26: 113(李忠文, 赵明久, 戎利建. 沉淀强化奥氏体合金的氢致断裂行为[J]. 材料研究学报, 2012, 26: 113)
[12]
Chen S H, Zhao M J, Rong L J.Hydrogen-induced cracking behavior of twin boundary in γ′ phase strengthened Fe-Ni based austenitic alloys[J]. Mater. Sci. Eng., 2013, A561: 7
[13]
Zhou B X, Liu W Q.The application of 3DAP in the study of materials science[J]. Mater. Sci. Tech., 2007, 15: 405(周邦新, 刘文庆. 三维原子探针及其在材料科学研究中的应用[J]. 材料科学与工艺, 2007, 15: 405)
[14]
Marquis E A, Bachhav M, Chen Y M, et al.On the current role of atom probe tomography in materials characterization and materials science[J]. Curr. Opin. Solid State Mater. Sci., 2013, 17: 217
[15]
Kapoor M, Isheim D, Ghosh G, et al.Aging characteristics and mechanical properties of 1600 MPa body-centered cubic Cu and B2-NiAl precipitation-strengthened ferritic steel[J]. Acta Mater., 2014, 73: 56
[16]
Jiao Z B, Luan J H, Miller M K, et al.Effects of Mn partitioning on nanoscale precipitation and mechanical properties of ferritic steels strengthened by NiAl nanoparticles[J]. Acta Mater., 2015, 84: 283
[17]
Baik S I, Rawlings M J S, Dunand D C. Atom probe tomography study of Fe-Ni-Al-Cr-Ti ferritic steels with hierarchically-structured precipitates[J]. Acta Mater., 2018, 144: 707
[18]
Jiang S H, Wang H, Wu Y, et al.Ultrastrong steel via minimal lattice misfit and high-density nanoprecipitation[J]. Nature, 2017, 544: 460
[19]
Bagot P A J, Silk O B W, Douglas J O, et al. An atom probe tomography study of site preference and partitioning in a nickel-based superalloy[J]. Acta Mater., 2017, 125: 156
[20]
Meher S, Banerjee R.Partitioning and site occupancy of Ta and Mo in Co-base γ/γ′ alloys studied by atom probe tomography[J]. Intermetallics, 2014, 49: 138
[21]
Huang Y Y, Mao Z G, Noebe R D, et al.The effects of refractory elements on Ni-excesses and Ni-depletions at γ (f.c.c.)/γ′(L12) interfaces in model Ni-based superalloys: Atom-probe tomographic experiments and first-principles calculations[J]. Acta Mater., 2016, 121: 288
[22]
Hwang J Y, Nag S, Singh A R P, et al. Evolution of the γ/γ' interface width in a commercial nickel base superalloy studied by three-dimensional atom probe tomography[J]. Scr. Mater., 2009, 61: 92
[23]
Tan X P, Mangelinck D, Perrin-Pellegrino C, et al.Atom probe tomography of secondary γ' precipitation in a single crystal Ni-based superalloy after isothermal aging at 1100 ℃[J]. J. Alloys Compd., 2014, 611: 389
[24]
Miller M K.Atom Probe Tomography: Analysis at the Atomic Level[M]. New York: Kluwer Academic/Plenum Publishers, 2000: 11, 160
[25]
Larson D J, Prosa T J, Ulfig R M, et al.Local Electrode Atom Probe Tomography [M]. New York: Spring Press, 2013: 180
[26]
Yeli G, Auger M A, Wilford K, et al.Sequential nucleation of phases in a 17-4PH steel: Microstructural characterisation and mechanical properties[J]. Acta Mater., 2017, 125: 38
[27]
Rhodes C G, Thompson A W.Microstructure and hydrogen performance of alloy-903[J]. Metall. Trans., 1977, 8A: 949
[28]
Reed R C.The Superalloys: Fundamentals and Applications [M]. Cambridge: Cambridge University Press, 2006: 43
[29]
Hornbogen E, Gahr K H Z. Distribution of plastic strain in alloys containing small particles[J]. Metallography, 1975, 8: 181