Please wait a minute...
Acta Metall Sin  2018, Vol. 54 Issue (10): 1435-1441    DOI: 10.11900/0412.1961.2018.00013
Current Issue | Archive | Adv Search |
Grain Orientation Competitive Growth of High Melting Point Metals Ir and Mo Under Electron Beam Floating Zone Melting
Shuangming LI1(), Binqiang WANG1, Zhenpeng LIU1, Hong ZHONG1, Rui HU1, Yi LIU2, Ximing LUO2
1 State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
2 Kunming Institute of Precious Metals, Kunming 650106, China
Cite this article: 

Shuangming LI, Binqiang WANG, Zhenpeng LIU, Hong ZHONG, Rui HU, Yi LIU, Ximing LUO. Grain Orientation Competitive Growth of High Melting Point Metals Ir and Mo Under Electron Beam Floating Zone Melting. Acta Metall Sin, 2018, 54(10): 1435-1441.

Download:  HTML  PDF(2856KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The preparation of single crystal involves the grain orientation competitive growth. For high melting point metals, Mo is a typical bcc crystal structure and its preferred growth orientation of single crystal was revealed to be the [110] direction, different from the known preferred growth orientation [100] for bcc metals during solidification. This disagreement remains unclear. For the high melting point metal Ir that is a fcc crystal structure, its preferred growth orientation of single crystal remains unknown. Based on electron beam floating zone melting (EBFZM), the orientation competitive growth of these two metals Mo and Ir with three different directions [100], [110] and [111] has been analyzed using solidification theory. It shows that the preferred growth orientation of Mo is the [110] direction at a planar front interface. When introducing the interface energy anisotropy, the preferred growth orientation of Mo could be the [100] or the [110] direction, depending on the magnitude of interface energy anisotropy parameters a1 and a2. This result matches well with the experimental results of Mo single crystal prepared by EBFZM. For the fcc structure Ir, its preferred growth orientation always keeps the [100] direction, agreeing with the experimental results of Ir single crystal prepared by EBFZM in this study. Besides, the effects of interface curvature undercooling and kinetic undercooling on the growth behavior of single-crystal metals prepared by EBFZM have been discussed. It demonstrates that when the grain size in the specimen is in the order of about millimeter or less, the curvature undercooling would dominate the grain orientation competitive growth. As the grain size becomes in the order of about centimeter or larger, the kinetic undercooling would prefer the grain competitive growth process.

Key words:  electron beam floating zone melting      grain orientation competitive growth      interface energy anisotropy      preferred growth direction     
Received:  10 January 2018     
ZTFLH:  TG292  
Fund: Supported by National Natural Science Foundation of China-Yunnan Province Joint Fund (No.U1202273) and National Natural Science Foundation of China (No.51774239)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2018.00013     OR     https://www.ams.org.cn/EN/Y2018/V54/I10/1435

Fig.1  Relationships between the kinetic undercooling (ΔTk) and growth rate (V) for pure metals Ir (a) and Mo (b) prepared by electron beam floating zone melting (EBFZM)
Fig.2  Values of interface energy anisotropy parameters (a1 and a2) for Mo and some selected fcc metals (Where the data are taken from the Ref.[17], d[100] and d[110] are the interface stiffness of two different orientations [100] and [110], respectively)
Fig.3  Curvature undercooling (ΔTr) as a function of curvature radius (r) for Ir and Mo with different a1 and a2
(a) only considering a1 for Ir
(b) considering a1 and a2 for Ir
(c) only considering a1 for Mo
(d) considering a1 and a2 for Mo
Fig.4  Relationships between V and r at ΔTr=ΔTk for Ir (a) and Mo (b) prepared by EBFZM
Fig.5  Grain evolution of Ir prepared by EBFZM (a~d), XRD spectrum (e) and Laue diffraction pattern of single crystal in Fig.5d (f)
[1] Kenji A.Why do we study ultra-high purity base metals?[J]. Mater. Trans., JIM, 2000, 41: 233
[2] Yang B C, Hu Y D, Cui H L.Trend in development and applications of sputtering target materials[J]. Vacuum, 2002, (1): 1(杨邦朝, 胡永达, 崔红玲. 溅射靶材的应用及发展趋势[J]. 真空, 2002, (1): 1)
[3] Duffar T.Crystal Growth Processes Based on Capillarity: Czochralski, Floating Zone, Shaping and Crucible Techniques[M]. Chichester: John Wiley & Sons Ltd, 2010: 204
[4] Glebovsky V G, Semenov V N, Lomeyko V V.The characteristic features of growth and the real structure of tungsten tube crystals[J]. J. Cryst. Growth, 1989, 98: 487
[5] Zhang J, Shu D, Rao Q L, et al.Nucleation and growth of high purity aluminum grains in directional solidification bulk sample without electromagnetic stirring[J]. Trans. Nonferrous Met. Soc. China, 2006, 16: 1
[6] Xu Z M, Guo Z Q, Li J G.A new method to evaluate the quality of single crystal Cu by an X-ray diffraction butterfly pattern method[J]. Mater. Charact., 2004, 53: 395
[7] Lee D N, Kim K H, Lee Y G, et al.Factors determining crystal orientation of dendritic growth during solidification[J]. Mater. Chem. Phys., 1997, 47: 154
[8] Hu Z W, Li Z K, Zhang Q, et al.Progress on single crystals of refractory metals of their alloys[J]. Rare Met. Mater. Eng., 2007, 36: 367(胡忠武, 李中奎, 张清等. 难熔金属及其合金单晶的发展[J]. 稀有金属材料与工程, 2007, 36: 367)
[9] Xiao D C, Li C Y, Ying T R, et al.Preparation of niobium single crystals with floating zone melting technique and a discussion on its mechanism[J]. Shanghai Met.(Nonferrous Met.), 1983, 4(2): 11(肖德传, 李长英, 应铁如等. 悬浮区熔法制取铌单晶及其机理探讨[J]. 上海金属(有色分册), 1983, 4(2): 11)
[10] Stefanescu D M.Science and Engineering of Casting Solidification [M]. 3rd Ed., Switzerland: Springer International Publishing, 2015: 157
[11] Gonzales F, Rappaz M.Dendrite growth directions in aluminum-zinc alloys[J]. Metall. Mater. Trans., 2006, 37A: 2797
[12] Dantzig J A, Di Napoli P, Friedli J, et al.Dendritic growth morphologies in Al-Zn alloys—Part II: Phase-field computations[J]. Metall. Mater. Trans., 2013, 44A: 5532
[13] Haxhimali T, Karma A, Gonzales F, et al.Orientation selection in dendritic evolution[J]. Nat. Mater., 2006, 5: 660
[14] Verstraete M J, Charlier J C.Why is iridium the best substrate for single crystal diamond growth?[J]. Appl. Phys. Lett., 2005, 86: 191917
[15] Glebovsky V G, Semenov V N.Growing single crystals of high-purity refractory metals by electron-beam zone melting[J]. High Temp. Mater. Proc., 1995, 14: 121
[16] Cawkwell M J, Nguyen-Manh M, Woodward C, et al.Origin of brittle cleavage in iridium[J]. Science, 2005, 309: 1059
[17] Hoyt J J, Asta M, Sun D Y.Molecular dynamics simulations of the crystal-melt interfacial free energy and mobility in Mo and V[J]. Philos. Mag., 2006, 86: 3651
[18] Amini M, Laird B B.Kinetic coefficient for hard-sphere crystal growth from the melt[J]. Phys. Rev. Lett., 2006, 97: 216102
[19] Jiang Q, Lu H M.Size dependent interface energy and its applications[J]. Surf. Sci. Rep., 2008, 63: 427
[20] Zee R H, Xiao Z, Chin B A, et al.Processing of single crystals for high temperature applications[J]. J. Mater. Proc. Technol., 2001, 113: 75
[21] Napolitano R E, Liu S, Trivedi R.Experimental measurement of anisotropy in crystal-melt interfacial energy[J]. Interface Sci., 2002, 10: 217
[22] Keene B J.Review of data for the surface tension of pure metals[J]. Int. Mater. Rev., 1993, 38: 157
[23] Wang H.Research on the technology of molybdenum crystals of refractory metals prepared by electron beam floating zone melting [D]. Xi'an: Northwestern Polytechnical University, 2007(王红. 难熔金属钼晶体的电子束悬浮区熔定向凝固工艺研究 [D]. 西安: 西北工业大学, 2007)
[24] Li S M, Geng Z B, Hu R, et al.Effect of growth angle and solidification rate on the floating zone stability for processing of high-temperature pure metals[J]. Acta Metall. Sin., 2015, 51: 114(李双明, 耿振博, 胡锐等. 高熔点金属区域熔炼中晶体生长角和凝固速率对熔区稳定性的影响[J]. 金属学报, 2015, 51: 114)
[25] Yang J R, Wang H, Wang B Q, et al.Numerical and experimental study of electron beam floating zone melting of Iridium single crystal[J]. J. Mater. Proc. Technol., 2017, 250: 239
[1] PENG Dongjian, LIN Xin, ZHANG Yunpeng, GUO Xiong, WANG Meng, HUANG Weidong. INVESTIGATION OF EFFECT OF INTERFACE ENERGY ANISOTROPY ON DENDRITIC GROWTH IN UNIDIRECTIONAL SOLIDIFICATION BY FRONT TRACKING SIMULATION[J]. 金属学报, 2013, 49(3): 365-371.
[2] YANG Mei WANG Gang TENG Chunyu XU Dongsheng ZHANG Jian YANG Rui WANG Yunzhi . 3D PHASE FIELD SIMULATION OF EFFECT OF INTERFACIAL ENERGY ANISOTROPY ON SIDEPLATE GROWTH IN Ti–6Al–4V[J]. 金属学报, 2012, 48(2): 148-158.
No Suggested Reading articles found!