| INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY |
Ju KANG1,2,Jichao LI2,Zhicao FENG2,Guisheng ZOU1,Guoqing WANG4,Aiping WU1,3( ) |
1 Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China 2 Fontana Corrosion Center, The Ohio State University, Columbus, Ohio 43210-1185, USA 3 State Key Laboratory of Tribology, Department of Mechanical Engineering, Tsinghua University, Beijing 100084, China 4 China Academy of Launch Vehicle Technology, Beijing 100076, China |
|
Cite this article:
Ju KANG,Jichao LI,Zhicao FENG,Guisheng ZOU,Guoqing WANG,Aiping WU. INVESTIGATION ON MECHANICAL AND STRESS CORROSION CRACKING PROPERTIES OF WEAKNESS ZONE IN FRICTION STIR WELDED 2219-T8 Al ALLOY. Acta Metall Sin, 2016, 52(1): 60-70.
|
|
|
Abstract Al alloy 2219 (AA2219) is widely used in the aerospace industry, and friction stir welding (FSW) is an ideal method to join it. The ultimate tensile strength of an FSW AA2219-T8 joint can be as high as 344 MPa which is significantly higher than that welded by other methods such as gas tungsten arc welding. However, the thermo-mechanically affected zone (TMAZ) in the FSW joints of AA2219-T6/T8 is a weakness zone of mechanical property and is susceptible to stress corrosion cracking (SCC), but the reasons are not been well understood. In this work, the mechanical and electrochemical properties of different zones in AA2219-T8 joints obtained by the FSW method were studied. The welding thermal cycles during welding were measured using an array of type K thermocouples. During the tensile process of the joints, digital image correlation (DIC) technique and high speed video technique were employed to investigate the deformational behavior and fracture pathway of the TMAZ, respectively. A microcell method was used to study the micro-electrochemical characteristics of the joints with and without stress. The results showed that the minimum strength located at a position where the weighted strengthening effects of both thermal cycles and stir action were the weakest. The DIC results revealed that the deformation concentrated mainly in the TMAZ during the tensile tests. However, due to the different restraints from the nugget zone (NZ) led to a large strain in the root side than that in the crown side. This made the root side susceptible to cracks initiation. In situ tensile testing indicated that cracks occurred only in the TMAZ at 190 MPa, indicating that the protective surface films in the TMAZ were more prone to crack than those in other zones of the joint. This led the TMAZ to be the weakest zone to pitting corrosion in an aggressive environment. Once pits generate in the TMAZ, the local stress will concentrate near the tip of the pitting, resulting in failure.
|
|
Received: 07 April 2015
|
| [1] | Xu W F, Liu J H, Luan G H, Dong C L. Acta Metall Sin, 2008; 44: 1404 | | [1] | (徐韦锋, 刘金合, 栾国红, 董春林. 金属学报, 2008; 44: 1404) | | [2] | Malarvizhi S, Balasubramanian V. Mater Des, 2011; 32: 1205 | | [3] | Mishra R S, Ma Z Y. Mater Sci Eng, 2005; R50: 1 | | [4] | Kang J, Fu R D, Luan G H, Dong C L, He M. Corros Sci, 2010; 52: 620 | | [5] | Liu H J, Zhang H J, Yu L. Mater Des, 2011; 32: 1548 | | [6] | Srinivasan P B, Arora K S, Dietzel W, Pandey S, Schaper M K. J Alloys Compd, 2010; 492: 631 | | [7] | Chen Y C, Feng J C, Liu H J. Mater Charact, 2009; 60: 476 | | [8] | Liu H J, Zhang H J, Huang Y X, Yu L. Trans Nonferrous Met Soc China, 2010; 20: 1387 | | [9] | Xu W F, Liu J H, Luan G H, Dong C L. Mater Des, 2009; 30: 3460 | | [10] | Paglia C S, Buchheit R G. Mater Sci Eng, 2006; A429: 107 | | [11] | Zhang H J, Liu H J, Yu L. Sci Technol Weld Joining, 2011; 16: 459 | | [12] | Zhang H J, Liu H J. Mater Des, 2013; 45: 206 | | [13] | Li J Q, Liu H J. Mater Des, 2013; 43: 299 | | [14] | Li J Q, Liu H J. Mater Des, 2013; 45: 148 | | [15] | Malarvizhi S, Balasubramanian V. Trans Nonferrous Met Soc China, 2011; 21: 962 | | [16] | Suter T, B?hni H. Electrochim Acta, 2001; 47: 191 | | [17] | Liu X D, Frankel G S, Zoofan B, Rokhlin S I. Corros Sci, 2004; 46: 405 | | [18] | Yang B C, Yan J H, Sutton M A, Reynolds A P. Mater Sci Eng, 2004; A364: 55 | | [19] | John M P. Metall Trans, 1981; 12A: 269 | | [20] | Xu W F, Liu J H, Luan G H, Dong C L. Acta Metall Sin, 2009; 45: 490 | | [20] | (徐韦锋, 刘金合, 栾国红, 董春林. 金属学报, 2009; 45: 490) | | [21] | Cui G R, Ma Z Y, Li S X. Acta Mater, 2009; 57: 5718 | | [22] | Kang J, Luan G H, Fu R D. Acta Metall Sin, 2011; 47: 224 | | [22] | (康 举, 栾国红, 付瑞东. 金属学报, 2011; 47: 224) | | [23] | Yan D Y, Shi Q Y, Wu A P, Juergen S, Zhang Z L. J Mech Eng, 2010; 46: 106 | | [23] | (鄢东洋, 史清宇, 吴爱萍, Juergen S, 张增磊. 机械工程学报, 2010; 46: 106) | | [24] | Lei X F, Deng Y, Yin Z M, Xu G F. J Mater Eng Perform, 2014; 23: 2149 | | [25] | Xu W F, Liu J H, Chen D L, Luan G H. Int J Adv Manuf Technol, 2014; 74: 209 | | [26] | Dai Q L, Liang Z F, Wu J J, Meng L C, Shi Q Y. Acta Metall Sin, 2014; 50: 587 | | [26] | (戴启雷, 梁志芳, 吴建军, 孟立春, 史清宇. 金属学报, 2014; 50: 587) | | [27] | Woo W, Balogh L, Ungar T, Choo H, Feng Z L. Mater Sci Eng, 2008; A498: 308 | | [28] | Du D X, Fu R D, Li Y J, Jing L, Ren Y B, Yang K. Mater Sci Eng, 2014; A616: 246 | | [29] | Baek Y, Frankel G S. J Electrochem Soc, 2003; 150B: 1 | | [30] | Kim Y, Buchheit R G. Electrochim Acta, 2007; 52: 2437 | | [31] | Garcia V S, Colin F, Skeldon P, Thompson G E, Bailey P, Noakes T C Q, Habazaki H, Shimizu K. J Electrochem Soc, 2004; 151B: 16 | | [32] | Ramgopal T, Frankel G S. Corrosion, 2001; 57: 702 | | [33] | Muller I L, Galvele J R. Corros Sci, 1977; 17: 179 | | [34] | Newman R C, Healey C. Corros Sci, 2007; 49: 4040 | | [35] | Feng Z, Frankel G S, Matzdorf C A. J Electrochem Soc, 2014; 161C: 42 | | [36] | Feng Z, Boerstler J, Frankel G S, Matzdorf C A. Corrosion, 2015; 71: 771 | | [37] | Uhlig H H. Corrosion and Corrosion Control: an Introduction to Corrosion Science and Engineering. New York: John Wiley & Sons Inc, 1971: 309 | | [38] | Birnbaum H K, Sofronis P. Mater Sci Eng, 1994; A176: 191 |
|