Lü Baochen LIU Haitao REN Xin WANG Xiaoliang LI Gang SUN Yuejun. AN ATOM DENSE PACKING MODEL FOR METALLIC GLASS WITH HIGH SOLUTE CONCENTRATION IN (PSEUDO–) TERNARY SYSTEMS. Acta Metall Sin, 2012, 48(2): 240-244.
Abstract A modified Miracle model based on packing different atoms on the first shell of solute–centered cluster is advanced to predict the best glass–former in some high content (pseudo–) ternary systems such as Ti–Ni–Al etc. The calculated results not only for the best ribbon metallic glass–formers in Ti–Ni–Al, Ti–Ni–Sn, but also for the best bulk metallic glass–formers in some other systems correspond to the experimental results very well, indicating the validity of this model.