RESEACH ON LUBRICATION IN HOT EXTRUSION OF G3 CORROSION RESISTANT Ni–BASED ALLOY TUBE II. Calculation and Application of Glass Lubricant Viscosity–Composition
LIN Ben, WANG Baoshun, ZHANG Maicang, DONG Jianxin
School of Materials Science and Engineering, University of Science and Technology Beijing, Beijing, 100083
Cite this article:
LIN Ben WANG Baoshun ZHANG Maicang DONG Jianxin. RESEACH ON LUBRICATION IN HOT EXTRUSION OF G3 CORROSION RESISTANT Ni–BASED ALLOY TUBE II. Calculation and Application of Glass Lubricant Viscosity–Composition. Acta Metall Sin, 2011, 47(3): 374-379.
Abstract Based on the classical first–order mixture method which describes the relationship between the property value and component, a modified mixture method for predicting the viscosity property of borosilicate glass lubricant used in the hot extrusion of G3 alloy was established. Then, the viscosity properties of 10 different borosilicate glasses were predicted using this method. The viscosity data predicted by this calculation method coincided well with the experimental data, which showed that the calculaton model was of strong reliability. Therefore, according to this model, the glass composition could be reversely designed, which will assure the viscosity of glass to meet the requirements of glass lubricated hot extrusion of G3 alloy which has beeraised in the first article. It provides theoetical guidance for the design and preparation of glass lubrcant in the glass lbricated hot extrusion of G3 alloy.
SHUI Jiapeng; WANG Yulin (Laboratory of Internal Friction and Defects in Solids;Institute of Solid State Physics; Chinese Academy of Sctences; Hefei 230031). VISCOUS FLOW BEHAVIOUR OF AMORPHOUS Pd-Cu-SiALLOY[J]. 金属学报, 1996, 32(11): 1215-1220.
[13]
GUO Wenquan;WANG Jingtang Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang. ON THE ADOPTION OF λ_0 VALUE FOR ROSCOE'S EQUATION[J]. 金属学报, 1992, 28(4): 17-20.