THE MICRO–FABRICATING PROCESS AND ELECTROMAGNETIC PROPERTIES OF TWO KINDS OF Fe POWDERS WITH DIFFERENT GRAIN SIZES AND INTERNAL STRAINS
ZHOU Jing, WANG Wei, SUN Zhigang, GUAN Jianguo
State Key Laboratory of Advanced Technology for Materials Synthesis and Processing, Wuhan University of Technology, Wuhan 430070
Cite this article: 

ZHOU Jing WANG Wei SUN Zhigang GUAN Jianguo. THE MICRO–FABRICATING PROCESS AND ELECTROMAGNETIC PROPERTIES OF TWO KINDS OF Fe POWDERS WITH DIFFERENT GRAIN SIZES AND INTERNAL STRAINS. Acta Metall Sin, 2010, 46(8): 967-972.

Download:  PDF(2015KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The micro–fabricating process and electromagnetic properties of two kinds of Fe powders with different grain sizes and internal strains were studied. The results show that the homemade Fe powders with smaller grain size, larger internal strain and surface roughness than the carbonyl Fe powders, evolve into big and thin Fe flakes by micro–fabricating for 10 h with the help of the process control agent (PCA). When micro–fabrication for t=12 h, these Fe flakes will fracture and their average width will reduce due to strong internal strain. When t is further prolonged to 24 h, these Fe flakes become thinner, finally, those with larger aspect ratio and smaller width can be obtained, which show high permeability and low permittivity. The epoxy resin-based microwave absorbing materials containing such Fe flakes of 20% (volume fraction) exhibit a reflection loss less than −10 dB in the 9.4—17.9 GHz frequency range with a minimal peak of −14.6 dB, whose average thickness is 1.5 mm.

Key words:  Fe flake      micro–fabrication      electromagnetic parameter      microwave absorbing properties     
Received:  10 March 2010     
Fund: 

Supported by National High Technology Research and Development Program of China (No.2006AA03A209) and Young Teachers from Fok Ying Tung Education Foundation (No.101049)

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2010.00117     OR     https://www.ams.org.cn/EN/Y2010/V46/I8/967

[1] Walser R M, Win W, Valanju P M. IEEE Trans Magn, 1998; 34: 1390
[2] Deng L J, Zhou P H, Xie J L, Zhang L. J Appl Phys, 2007; 101: 103916
[3] Zhou P H, Deng L J, Xie J L, Liang D F. J Alloys Compd, 2008; 448: 303
[4] Xian W, Gong R Z, Li P G, Liu L Y, Cheng W M. Mater Sci Eng, 2007; 466A: 178
[5] Cho E K, Kwon H T, Cho E M, Song Y S, Sohn K Y, Park W W. Mater Sci Eng, 2007; A449–451: 368
[6] Zhang B S, Lu G, Feng Y, Xiong J, Lu H X. J Magn Magn Mater, 2006; 299: 205
[7] Moon B G, Sohn K Y, Park W W, Lee T D. Mater Sci Eng, 2007; A449–451: 426
[8] Huang J J. PhD Thesis, Lanzhou University, 2007
(黄娟娟. 兰州大学博士学位论文, 2007)
[9] Zhang X N. PhD Thesis, Beijing Institute of Technology, 2003
(张晓宁. 北京工业大学博士学位论文, 2003)
[10] Nie Y, He H H, Zhao Z S, Gong R Z, Yu H B. J Magn Magn Mater, 2006; 306: 125
[11] Dong D M, Guan J G,WangW, LiW, Zhou J. Acta Metall Sin, 2009; 45: 1141
(董德明, 官建国, 王维, 李维, 周静. 金属学报, 2009; 45: 1141)
[12] Wang Q, Guan J G, Liu S Q,Wang W, Zhang Q J. J Alloy Compd, 2006; 413: 155
[13] Tong G X,Wang W, Guan J G, Zhang Q J. J Inorg Mater, 2006; 21: 1461
(童国秀, 王维, 官建国, 张清杰. 无机材料学报, 2006; 21: 1461)
[14] Fan X A, Guan J G, Li Z Z, Mou F Z, Tong G X, Wang W. J Mater Chem, 2010; 20: 1676
[15] Pan J S, Tong J M, Tian M B. Material Science. 6th ed, Beijing: Tsinghua University Press, 1998: 205
(潘金生, 仝健民, 田民波. 材料科学基础. 第6版, 北京: 清华大学出版社, 1998: 205)
[16] Chen Z H, Chen D. Mechanical Alloying and Solid–Liquid Reaction Milling. 4th ed, Beijing: Chemical Industry Press, 2006: 58
(陈振华, 陈鼎. 机械合金化与固液反应球磨. 第4版, 北京: 化学工业出版社, 2006: 58)
[17] Fan X A, Guan J G, Wang W, Tong G X. J Phys, 2009; 42D: 075006

[1] Yuqiu CHEN, Yapei ZU, Jun GONG, Cao SUN, Chen WANG. Effect of Al Film on the Electromagnetic Properties of Glass Fiber Reinforced Resin Matrix Composite[J]. 金属学报, 2017, 53(11): 1511-1520.
[2] DONG Deming GUAN Jianguo WANG Wei LI Wei ZHOU Jing. PREPARATION AND ELECTROMAGNETIC PROPERTIES OF MICROMETER Fe FLAKES MODIFIED WITH EPOXY RESIN[J]. 金属学报, 2009, 45(9): 1141-1145.
No Suggested Reading articles found!