THEORETICAL ANALYSIS ON EFFECT OF TRANSFERENCE VELOCITY ON STRUCTURE OF POROUS METALS FABRICATED BY CONTINUOUS CASTING GASAR PROCESS
LIU Yuan1; LI Yanxiang1; LIU Runfa1;ZHOU Rong2; JIANG Yehua2; LI Zhenhua2
1.Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing 100084
2.Faculty of Mechanical and Electrical Engineering; Kunming University of Science and Technology; Kunming 650093
Cite this article: 

LIU Yuan LI Yanxiang LIU Runfa ZHOU Rong JIANG Yehua LI Zhenhua. THEORETICAL ANALYSIS ON EFFECT OF TRANSFERENCE VELOCITY ON STRUCTURE OF POROUS METALS FABRICATED BY CONTINUOUS CASTING GASAR PROCESS. Acta Metall Sin, 2010, 46(2): 129-134.

Download:  PDF(1629KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Transference velocity is an important processing parameter to influence the final lotus–type porous structure fabricaed by continuus casting Gasar process. Via solving the solute diffusion equation, a theoretical model was developed to predict the effect of the transference velocity on the porosity, the pore diameter and the inter–pore spacing. The predicted values at different transference velocities have a good agreement with the corresponding experimental results obtained by Japanese esearcher. The average pore diameter and the inter–pore spacing L both have a prominent decrease with the increase of transference velocity v, but the porosity only has a slight decrease. The theoretical relationships between the pore radius rg, the inter–pore spacing and the transference velocity can be described by the two simple equations as r1.72g ·v = A and L1.72 ·v = B, where A and B are all constants depending on the used gas presures and the melt temperature.

Key words:  porous metal      metal–gas eutectic      continuucasting      transference velocity     
Received:  31 July 2009     
Fund: 

Supported by National Natural Science Foundation of China and Yunnan Provincial Government (No.u0837603), Natural Science Foundation of Beijing (No.2092017), Scientific Research Foundation for the Returned Overseas Chinese Scholars, State Education Ministry (No.20091020471) and Key Talents Foundation of Tsinghua University

URL: 

https://www.ams.org.cn/EN/10.3724/SP.J.1037.2009.00527     OR     https://www.ams.org.cn/EN/Y2010/V46/I2/129

[1] Banhart J. Prog Mater Sci, 2001; 46: 559
[2] Shapovalov V I. US Pat, No.5181549, 1993
[3] Shapovalov V I. Mater Res Soc Symp Proc, 1998; 521: 281
[4] Nakajima H, Hyun S K, Ohashi K. Colloids Surf, 2001;179A: 209
[5] Yamamura S, Shiota H, Murakami K, Nakajima H. Mater Sci Eng, 2003; A318: 137
[6] Nakajima H, Lkeda T, Hyun S K. Adv Eng Mater, 2004; 6: 377
[7] Paradies C J, Tobin A. Mater Res Soc Symp Proc, 1998; 521: 297
[8] Apprill J M, Poirier D R, Maguire M C. Mater Res Soc Symp Proc, 1998; 521: 291
[9] Wolla J M. Mater Res Soc Symp Proc, 1995; 371: 377
[10] Liu Y, Li Y X, Zhang H W. Metall Trans, 2006; 37A: 2871
[11] Liu Y, Li Y X, Zhang H W. J Mater Sci Technol, 2006; 22: 306
[12] Liu Y, Li Y X, Wan J. Mater Sci Eng, 2005; A402: 47
[13] Liu Y, Li Y X. Trans Nonferrous Met Soc China, 2003; 13: 830
[14] Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004; 40: 1121
(刘 源, 李言祥, 张华伟. 金属学报, 2004; 40: 1121)
[15] Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2005; 41:886
(刘源, 李言祥, 张华伟. 金属学报, 2005; 41: 886)
[16] Park J S, Hyun S K, Suzuki S, Nakajima H. Acta Mater, 2007; 55: 5646
[17] Jackson K A, Hunt J D. Trans Metall Soc AIME, 1966; 236: 1129
[18] Hu H Q. Solidification Foundation. 2th Ed., Beijing: Mechanical Industry Press, 2000: 114, 175
(胡汉起. 金属凝固原理 (第2版). 北京: 机械工业出版社, 2000: 114, 175)
[19] An G Y. Formation Theory of Castings. Beijing: Mechanical Industry Press, 1989: 173
(安阁英. 铸件形成理论. 北京: 机械工业出版社, 1989: 173)
[20] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2005; 41: 55
(张华伟, 李言祥, 刘 源. 金属学报, 2005; 41: 55)
[21] Fisher D J. Hydrogen Diffusion in Metals: A 30–Year Retrospective. Scitec Publications Ltd., Switzerland, 1999: 55
[22] Jones H. Mater Lett, 2002; 53: 364

[1] XU Wence, CUI Zhenduo, ZHU Shengli. Recent Advances in Open-Cell Porous Metal Materials for Electrocatalytic and Biomedical Applications[J]. 金属学报, 2022, 58(12): 1527-1544.
[2] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[3] Yanxiang LI, Xiaobang LIU. Directionally Solidified Porous Metals: A Review[J]. 金属学报, 2018, 54(5): 727-741.
[4] LI Zaijiu, JIN Qinglin, YANG Tianwu, ZHOU Rong, JIANG Yehua. A THERMODYNAMIC MODEL FOR DIRECTIONAL SOLIDIFICATION OF METAL-HYDROGEN EUTECTIC[J]. 金属学报, 2014, 50(4): 507-514.
[5] CHEN Liutao ZHANG Huawei LIU Yuan LI Yanxiang. EXPERIMENTAL RESEARCH ON HEAT TRANSFER PERFORMANCE OF DIRECTIOANLLY SOLIDIFIED POROUS COPPER HEAT SINK[J]. 金属学报, 2012, 48(3): 329-333.
[6] CHEN Liutao ZHANG Huawei LIU Yuan LI Yanxiang. THEORETICAL STUDY ON HEAT TRANSFER PERFORMANCE OF DIRECTIOANLLY SOLIDIFIED POROUS COPPER HEAT SINK[J]. 金属学报, 2012, 48(11): 1374-1380.
[7] . Effect of Transverse Convection Induced by Density Differences on Bidirectional Solidification of Metal-Gas Eutectic[J]. 金属学报, 2008, 44(9): 1057-1062 .
[8] Hua-Wei ZHANG. The Critical Processing Conditions for Directional Solidification of Solid/Gas Eutectics[J]. 金属学报, 2007, 43(6): 589-594 .
[9] Hua-Wei ZHANG. Hydrogen Solubility in Pure Metals for Gasar Process[J]. 金属学报, 2007, 43(2): 113-118 .
[10] Hua-Wei ZHANG. Difficulty in Fabricating Lotus-type Porous Al by Gasar Process[J]. 金属学报, 2007, 42(1): 11-16 .
[11] QIU K Q. FABRICATION OF Zr41.25Ti13.75Ni10Cu12.5Be22.5 BULK METALLIC GLASS FOAM[J]. 金属学报, 2006, 42(4): 379-382 .
[12] ZHANG Huawei; LI Yanxiang; LIU Yuan. Gas Pressure Condition for Obtaining Uniform Lotus--Type Porous Structure by Gasar Process[J]. 金属学报, 2006, 42(11): 1171-1176 .
[13] ZHANG Huawei; LI Yanxiang; LIU Yuan. Evaluation of Porosity in Lotus--Type Porous Cu Fabricated with Gasar Process[J]. 金属学报, 2006, 42(11): 1165-1170 .
[14] Yuan Liu. Fabrication of Regular Porous Magnesium with Radial Pore Distribution[J]. 金属学报, 2006, 42(10): 1075-1080 .
[15] LIU Yuan; LI Yanxiang; ZHANG Huawei. FABRICATION OF LOTUS--STRUCTURED POROUS MAGNESIUM WITH GASAR PROCESS[J]. 金属学报, 2004, 40(11): 1121-1126 .
No Suggested Reading articles found!