| [1] David A L, Ray M H. Light Met Age, 1991; 2(9): 11
[2] Wang H B, Huang J F, Yang B. Mater Rev, 2003; 17(9):1
(王洪斌, 黄进峰, 杨 滨. 材料导报, 2003; 17(9): 1)
[3] Ferrer C P, Koul M G, Connolly B J, Moran A L. Corrosion, 2003; 59: 520
[4] Ramgopal T, Gouma P L, Frankel G S. Corrosion, 2002;58: 687
[5] Liu Y. J Beijing Union Univ(Nat Sci), 2006; 20(1): 31
(刘 洋. 北京联合大学学报(自然科学版), 2006; 20(1): 31)
[6] Lu H. PhD Thesis, University of Science and Technology Beijing, 1998
(吕 宏. 北京科技大学博士学位论文, 1998)
[7] Huang X Y, Li Y H, Xiao J M. J Chin Soc Corros Prot,1984; 4(1): 42
(黄显亚, 李永洪, 肖纪美. 中国腐蚀与防护学报, 1984; 4(1): 42)
[8] Najjar D, Magnin T, Waner T J. Mater Sci Eng, 1997,A238: 293
[9] Xiao S X, Wang C Y, Chen T L. The Application of the Discrete Variational Method in the Density Functional Theory to Chemistry and Materials Physics. Beijing: Science Press, 1998: 92
(肖慎修, 王崇愚, 陈天朗. 密度泛函理论的离散变分方法在化学和材料物理学中的应用. 北京: 科学出版社, 1998: 92 )
[10] Ashby M F. Philos Trans R Soc London, 1987; 393A: 322
[11] Zhou D W, Peng P, Liu J S. Sci China, 2006; 49E: 129
[12] Peng P, Han S C, Zheng C X, Liu R S, Jin T, Hu Z Q.Rear Met Mater Eng, 2005; 34: 854
(彭平, 韩绍昌, 郑采星, 刘让苏, 金涛, 胡壮麒. 稀有金 属材料与工程, 2005; 34: 854)
[13] Liu G L. Acta Phys Sin, 2006, 55: 1983
(刘贵立. 物理学报, 2006; 55: 1983)
[14] Liu G L, Li R D. Acta Phys Sin, 2006; 55: 776
(刘贵立, 李荣德. 物理学报, 2006; 55: 776)
[15] Haydock R. Solid State Physics. Vol.35, New York: Academic Press, 1980: 216
[16] Harrison W A. Electronic Structure and the Properties of Solids. San Francisco: Freeman, 1980: 551
[17] Slater J C, Koster G F. Phys Rev, 1954; 94: 1498
[18] Wang L G, Wang C Y. Mater Sci Eng, 1997; A234–236: 52
[19] Gruhl W. Aluminum, 1978; 54: 323
[20] Fan X G, Jiang D M, Shan C Z. Light Alloys Process Technol, 2006; 34(2): 31
(樊喜刚, 蒋大鸣, 单长智. 轻合金加工技术, 2006; 34(2): 31)
[21] Liu X Y, Xu W, Foiles S M, Adams J B. Appl Phys Lett, 1998; 72: 1578
[22] Liu X G, Wang X W, Wang J Y, Zhang H Y. J Phys: Condens Matter, 2005; 17: 4301
[23] Hu Q M, Xu D S, Li D. Acta Metall Sin, 2002; 38(Suppl. 1): 562
(胡青苗, 徐东升, 李 \ \ 东. 金属学报, 2002; 38(增刊 1): 562)
[24] Malis T, Chaturvedi M C. J Mater Sci, 1982; 17: 1479
[25] Zeng Y, Yin Z M, Pan Q L. J Cent South Univ Technol, 2002; 33: 592
(曾渝, 尹志民, 潘青林. 中南工业大学学报, 2002; 33: 592)
[26] Liu X G, Wang X W, Wang J Y, Zhang H Y. J Mater Sci Technol, 2006; 22: 135 |