| EIS STUDY ON THE EFFECTS OF HEAT TREATMENT ON CORROSION BEHAVIOR OF NICKEL BASE ALLOY COATING |
| ;Yong Wang |
| 中国石油大学 |
|
Cite this article:
Yong Wang. EIS STUDY ON THE EFFECTS OF HEAT TREATMENT ON CORROSION BEHAVIOR OF NICKEL BASE ALLOY COATING. Acta Metall Sin, 2008, 44(9): 1125-1130 .
|
|
|
Abstract NiCrBSi alloy powders were sprayed on a low carbon steel substrate using High velocity oxy-fuel (HVOF) spraying technique and then the samples with coating were heat treated in air furnace for 2h or 10min at 900°C. The corrosion failure process and corrosion resistance of coatings in 3.5% NaCl aqueous solution were investigated by using Electrochemical Impedance Spectroscope (EIS). EIS data shows that the as-sprayed coating cannot resist the penetration of corrosive solution and after 20h the steel substrate begins to be corroded. Local corrosion happens in 2h heat-treated coating if contacting coating with brine longer than 15h, while shape of EIS plots can hold stable for a long time and uniform corrosion happens in 10min heat-treated coating. Relationship of corrosion resistance with time for as-sprayed coating and heat-treated coatings in 3.5% NaCl was obtained using equivalent circuits. The corrosion resistance of 10min heat-treated coating and resistance to penetration of aqueous medium are far better than of as-sprayed coating, but the corrosion resistance of heat-treated coatings with long holding time (2h) is inferior to that of as-sprayed coating. The reasons why heat treatment can change the corrosion behavior of sprayed coating were discussed by the aid of analyzing microstructure.
|
|
Received: 18 February 2008
|
|
|
[1]Zhao W M,Wang Y,Dong L X,Wu K Y,Xue J.Surf Coat Technol,2005;190:293 [2]Lee C H,Min K O.Surf Coat Technol,2000;132:49 [3]Blackford J R,Buckley R A,Jones H,Sellars C M,Mc- Cartney D G,Horlock A J.J Mater Sci,1998;33:4417 [4]Kim B H,Suhr D S.Mater Trans,2000;41:1657 [5]Otsubo F,Era H,Uchida T,Kishitake K.J Therm Spray Technol,2000;9:499 [6]Hamashima K,Shinozaki Y,Sasaki M.In,McKotch R A,Webb R,eds.,1997 Int Conf on Powder Metallurgy and Particulate Materials,Princeton,N J,Metal Powder Industries Fed,1997:243 [7]Okada R.J Jpn Inst Met,1997;61:625 (岡田亮二.日本金属学会志,1997;61:625) [8]Zhao W M,Wang Y,Xue J,Wu K Y.Acta Metall Sin, 2005;41:178 (赵卫民,王勇,薛锦,吴开源.金属学报,2005;41:178) [9]Zhao W M,Wang Y,Xue J,Wu K Y.Trans Chin Weld Inst,2005;26(1):41 (赵卫民,王勇,薛锦,吴开源.焊接学报,2005;26(1):41) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|