GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF LEAD ALLOY ANNEALED AT ELEVATED TEMPERATURE AFTER ROLLED AT DIFFERENT TEMPERATURES
;;;
山东理工大学机械工程学院金属材料系
Cite this article: 

;. GRAIN BOUNDARY CHARACTER DISTRIBUTIONS OF LEAD ALLOY ANNEALED AT ELEVATED TEMPERATURE AFTER ROLLED AT DIFFERENT TEMPERATURES. Acta Metall Sin, 2008, 44(6): 652-658 .

Download:  PDF(1980KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The grain boundary character distributions (GBCD) of Pb-0.09Ca-1.5Sn-0.026Al alloy (mass fraction, %) rolled at different temperatures and then annealed in the same way (270℃/10min) were investigated by means of electron back scatter diffraction (EBSD)techniques. The results showed that special boundaries such as ∑3, ∑9 and ∑27 were largely populated in the specimen which was rolled at room temperature and the temperature of liquid nitrogen(-196℃), the fraction of ∑3 and ∑9+∑27 boundaries exceeded 60% and 12%, respectively. The connectivity of general high angle boundaries (HABs) networks was interrupted substantially by special boundaries, indicating the optimization of GBCD was achieved. However, much lower fraction of special boundaries were developed in the specimen which were rolled at 100℃, and the connectivity of general high angle boundaries (HABs) network was not interrupted significantly, implying the GBCD was not optimized. Single section trace analysis based on EBSD technique revealed that incoherent 3 boundaries took the major parts of of 3 boundaries in the optimized GBCD
Key words:       
Received:  10 October 2007     
ZTFLH:  TG111  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I6/652

[1]Palumbo G,Erb u.MRS Bull,1999;24(11):27
[2]Wang W G,Zhou B x,Feng L,Zhang x,Xia s.Acta Metall Sin,2006:42:715 (王卫国,周邦新,冯柳,张欣,夏爽.金属学报,2006;42:715)
[3]Wang W G,Guo H.Mater Sci Eng,2007;A445-446:55
[4]Zhang X,Wang W G,Guo H,Jiang Y.Acta Metall Sin. 2007;43:454 (张欣,王卫国,郭红,姜英.金属学报,2007;43:454)
[5]Yu Y N.Metallic Theory.Beijing:Metallurgial Industry Press,2000:428 (余水宁.金属学原理.北京:冶金工业出版社,2000:428)
[6]Palumbo G,Aust K T,Erb U,King P J,Brennenstuhl A M,Lichtenberger P C.Phys Star Sol(a),1992;131:425
[7]Brandon D G.Acta Metall,1966;14:1479
[8]Randle V.Scr Mater,2001;44:2789
[9]Fang X Y,Wang W G,Guo H,Zhang X,Zhou B X.Acta Metall Sin,2007;43:1239 (方晓英,王卫国,郭红,张欣,周邦新.金属学报,2007;43:1239)
[10]Xia S,Zhou B X,Chen W J,Wang W G.Aeta Metall Sin, 2006;42:129 (夏爽,周邦新,陈文觉,王卫国.金属学报,2006;42:129)
[11]Schuh C A,Kumar M,King W E.J Mater Sci,2005;40: 847
[12]Mahajan S,Pande C S,Imam M A,Rath B B.Acta Mater, 1996;45:2633
[13]Randle V,Davies P,Hulm B.Philo Mag,1999;79A:305
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!