Modeling and optimization of movement parameters of reciprocating tubular spray depositing
南京航空航天大学 机电学院 210016
Cite this article: 

. Modeling and optimization of movement parameters of reciprocating tubular spray depositing. Acta Metall Sin, 2008, 44(4): 501-506 .

Download:  PDF(556KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Process principle of reciprocating spray forming large thick-wall tubular was analyzed. The distribution of the mass flux of spray cone and behavior of the deposit track of single layer were studied, a model of deposit of single layer was established on the basis of these research. Aiming at the model and the helix characteristic of the deposit track, the influences of model parameters (Mmax 、a 、d) and mandrel movement parameters (w、v) on the deposit behavior ,and the influences of mandrel radius on deposit thickness of single layer were analyzed. Through the simulating of the deposit thickness overlapped by the deposit profiles of multiple circumrotating cycles,the movement parameters(w、v)of tubular spray forming were optimized.
Key words:  reciprocating spray depositing      optimization of movement parameters      deposit track of single layer     
Received:  21 September 2007     
ZTFLH:  TG124  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I4/501

[1]Hattel J H,Pryds N H.Acta Mater,2004;52:5275
[2]Pryds N H,Hattel J H,Pedersen T B,Thorborg J.Acta Mater,2002;50:4075
[3]Hattel J H,Pryds N H,Pedersen T B.Mater Sci Eng, 2004;383:184
[4]Chaudhury S K,Singha A K,Sivaramakrishnana C S, Panigrahib S C.Mater Sci Eng,2005;A393:196
[5]Cao F Y,Cui C S,Fan H B,Li Q C.Chin J Nonferrous Met,1999;9:213 (曹福洋,崔成松,范洪波,李庆春.中国有色金属学报,1999;9:213)
[6]Cui C S,Fritsching U,Alwin S,Li Q C.Acta Mater,2005; 53:2765
[7]Cui C S,Fritsching U,Alwin S,Li Q C.Acta Mater,2005; 53:2775
[8]Chen Z H,Yan H G,Chen G,Zhang F Q,Hu Z X,Fu J X.J Hunan Univ(Nat Sci),2001;28(5):20 (陈振华,严红革,陈刚,张福全,胡仲勋,傅杰新.湖南大学学报(自然科学版),2001;28(5):20
[9]Chen Z H,Chen D,Kang Z T,Yan H G,Zhang F Q,Yuan W H,Wang H M.J Hunan Univ(Nat Sci),2002;29(6): 23 (陈振华,陈鼎,康智涛,严红革,张福全,袁武华,王慧敏.湖南大学学报(自然科学版),2002;29(6):23)
[10]Zhang H.CN Pat,03230878.7,2004 (张豪.中国专利,03230878.7,2004)
[11]Zhang H,Zhang D,Zhang J,Song L.CN Pat,03117066.8, 2004 (张豪,张荻,张捷,宋立.中国专利,03117066.8,2004)
[1] JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge. Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel[J]. 金属学报, 2022, 58(12): 1545-1556.
[2] W.P.Jia. The numerical simulation of interaction between melting pool and metal powder during laser rapid forming[J]. 金属学报, 2007, 43(5): 546-552 .
No Suggested Reading articles found!