| TRIBOLOGICAL PROPERTIES OF PLASMA SPRAYED FeS COMPOSITE COATINGS MIXED WITH NANO-SiC |
| Ye Pan;;; |
| 东南大学材料科学与工程系 |
|
Cite this article:
Ye Pan. TRIBOLOGICAL PROPERTIES OF PLASMA SPRAYED FeS COMPOSITE COATINGS MIXED WITH NANO-SiC. Acta Metall Sin, 2008, 44(4): 463-466 .
|
|
|
Abstract FeS/SiC composite coatings have been successfully produced by plasma spray technique. SiC particles with nano-scale are uniformly distributed in FeS matrix. There is a good bond between the coatings and 40Cr steel substrate. The tribological properties of FeS coating and FeS/SiC composite coatings have been investigated. The results show that FeS/SiC composite coatings have good antifriction and wear resistance properties. The friction coefficients of the composite coatings, mixed with nano SiC particles in weight fraction 0.2 and 0.3, are almost same as that of FeS coating under dry sliding, but the wear volume of them is remarkably decreased over the range of an order of magnitude. In oil lubrication, the friction coefficient of FeS/SiC composite coatings is smaller than that of FeS coating. So the composite coatings have superior antifriction property in the case.
|
|
Received: 20 March 2007
|
|
|
[1]Rapoport L,Leshinsky V,Lapsker I,Volovik Y,Nepom- nyashcky O,Lvovsky M,Popovitz-Biro R,Feldman Y, Tenne R.Wear,2003;255:785 [2]Wang H D,Zhuang D M,Wang K L,Liu J J,Fang X D, Li Y L.Aeta Metall Sin,2003;39:1031 (王海斗,庄大明,王昆林,刘家浚,方晓东,李永良.金属学报,2003;39:1031) [3]Chen Y X,Feng Z Z,Liu W M.Tribology,2002;22(2):85 (陈云霞,冯治中,刘维民.摩擦学学报,2002;22(2):85) [4]Lee I,Park I.Surf Coat Technol,2006;200:3540 [5]Chen Y X,Wang B,Liu W M.J Process Eng,2002;2: 365 (陈云霞,王博,刘维民.过程工程学报,2002;2:365) [6]Cosemans P,Zhu X,Gelis J P,Stappen M V.Surf Coat Technol,2003;174-175:416 [7]Goller R,Torri P,Baker M A,Gilmore R,Gissler W.Surf Coat Technol,1999;120-121:453 [8]Wang C M.Master Dissertation,Southeast University, Nanjing,2005 (王春明.东南大学硕士学位论文,南京,2005) [9]Xu T,Zhao J Z,Xu K.Tribol Trans,1997;40;178N |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|