EFFECT OF FRICTION STIR PROCESSING ON THE MICROSTRUCTURE OF CAST 7075 ALUMINUM ALLOY
Cite this article: 

. EFFECT OF FRICTION STIR PROCESSING ON THE MICROSTRUCTURE OF CAST 7075 ALUMINUM ALLOY. Acta Metall Sin, 2008, 44(3): 319-324 .

Download:  PDF(1462KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new processing technique - friction stir processing (FSP) - was applied to process cast 7075 aluminum alloy. The effect of processing parameters on the microstructure of the stir zone was investigated. Because the coarse grains and coarse second-phase particles at grain boundaries in cast 7075Al reduced its plastic deformation ability substantially, it was difficult to obtain a uniform microstructure by usual tool designs and processing parameters. By overlapping the FSP passes, the homogeneous and fine equiaxed grains were produced in the stir zone. Furthermore, reducing the tool size and increasing the rotation rate resulted in a significant improvement in the microstructural homogeneity of the stir zone.
Key words:       
Received:  13 September 2007     
ZTFLH:  TG146  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I3/319

[1]Mishra R S,Mahoney M W,McFadden S X,Mara N A, Mukherjee A K.Scr Mater,2000;42:163
[2]Mishra R S,Mahoney M W.Mater Sci Forum,2001;357- 359:507
[3]Mishra R S,Mahoney M W,McFadden S X,Mara N A, Mukherjee A K.Scr Mater,1999;42:163
[4]Ma Z Y,Mishra R S,Mahoney M W.Acta Mater,2002; 50:4419
[5]Ma Z Y,Mishra R S.Acta Mater,2003;51:3551
[6]Dutta A,Charit L,Johannes L B,Mishra R S.Mater Sci Eng,2005;A395:173
[7]Johannes L B,Mishra R S.Mater Sci Eng,2007;A464: 255
[8]Mishra R S.Adv Mater Processes,2004;162:45
[9]Ma ZY,Mishra RS,Mahoney M W.Scr Mater,2004;50: 931
[10]Charit I,Mishra R S.Acta Mater,2005;53:4211
[11]Johannes LB,Charit I,Mishra R S,Verma R.Mater Sci Eng,2007;A464:351
[12]Ma Z Y,Sharma S R,Mishra R S.Mater Sci Eng,2006; A433:269
[13]Arbegast W J,Hartley P J.In:Proce Fifith Int Conf of Trends in Welding Research,Pine Mounatain,GA,1998: 541
[14]Zhao Y H,Lin S B,Wu L,Qu F X.Mater Lett,2005;59: 2948
[15]Ma Z Y,Sharma S R,Mishra R S.Mater Sci Eng,2006; A433:269
[16]Elangovan K,Balasubramanian V.Mater Design,in press
[17]Su J Q,Nelson T W,Sterling C J.Mater Sci Eng,2005; A405:277
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!