INFLUNENCE OF MELT SUPERHEATING TIME ON THE SOLIDIFICATION MICROSTRUCTURE OF DD3 SINGLE CRYSTAL SUPERALLOY
ZOU Min-Ming;Jun Zhang;Lin LIU;
西北工业大学
Cite this article: 

ZOU Min-Ming; Jun Zhang; Lin LIU. INFLUNENCE OF MELT SUPERHEATING TIME ON THE SOLIDIFICATION MICROSTRUCTURE OF DD3 SINGLE CRYSTAL SUPERALLOY. Acta Metall Sin, 2008, 44(2): 155-158 .

Download:  PDF(380KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  26 June 2007     

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I2/155

[1]Gui Z L.Aviat Product Eng,1995;(4):12 (桂忠楼.航空制造工程,1995;(4):12)
[2]Kolotukhin E V,Baum B A,Kuleshova E A,Larioiov V N,Tretyakova E E,Tyagunov G V.Steel,1992;(7):21 (1992;(7):21)
[3]Wang Z,Li J G,Zhao N R,Jin T,Zhang J H.Acta Metall Sin,2002;38:920 (王震,李金国,赵乃仁,金涛,张静华.金属学报,2002;38:920)
[4]Chen G,Yu J W,Xie F Q,Fu H Z.Non-equilibrium Solid- ification of New Type Metallic Material.Beijing:Science Press,2004:205 (陈光,俞建威,谢发勤,傅恒志.非平衡凝固新型金属材料.北京:科学出版社.2004:205)
[5]Zou M M,Zhang Jun,Liu L,Fu H Z.Acta Metall Sin, 2008;44:59 (邹敏明,张军,刘林,傅恒志.金属学报,2008;44:59)
[6]Guo Z Q,Fu T,Wang N,Fu H Z.J Inorganic Mater, 2002;17:460 (郭振琪,付涛,王宁,傅恒志.无机材料学报,2002;17:460)
[7]Kattamis T Z,Flemings M C.TMS AIME,1965;233:992
[8]Liu L,Zhen B L,Banerji A,Reif W,Sommer F.Scr Metall Mater,1994;30:593
[9]Yin F S,Sun X F,Li J G,Guan H R,Hu Z Q.Scr Mater, 2003;48:425
[10]Chen C L,Lu F Y.Acta Metall Sin,1997;33:455 (陈长乐,陆富一.金属学报,1997;33:455)
[11]Chen G,Yu J W,Xie F Q,Fu H Z.Acta Metall Sin,2001; 37:488 (陈光,俞建威,谢发勤,博恒志.金属学报,2001;37:488)
[12]Yin F S,Sun X F,Guan H R,Hu Z Q.J Alloy Compd, 2004;364:225
[13]Huo Y P,Zheng J R.Non-equilibrium State Statistic The- ory.Beijing:Science Press,1987:371 (霍裕平,郑久仁.非平衡态统计理论.北京:科学出版社,1987:371)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!