| Effect of solute trapping on the growth process in undercooled eutectic melts |
| ;;;Yaohe Zhou |
| 上海交通大学 |
|
Cite this article:
Yaohe Zhou. Effect of solute trapping on the growth process in undercooled eutectic melts. Acta Metall Sin, 2008, 44(11): 1335-1339 .
|
|
|
Abstract Abstract:Considering the solute trapping in non-equilibrium rapid solidification, in this paper, we discuss the effect of solute trapping on the growth process basing on the existent eutectic models. It is found that the growth velocity is increased and lamellar spacing and dendritic tip radius are decreased, and the smaller the equilibrium solute partition coefficient, the more prominent the effect.
|
|
Received: 25 March 2008
|
|
|
[1]Jackson K A,Hunt J D.TMS AIME,1966;236:1129 [2]Trivedi R,Magnin P,Kurz W.Acta Metall,1987;35:971 [3]Li J F,Zhou Y H.Sci China,2005;35E:449 (李金富,周尧和.中国科学,2005;35E:449) [4]Kurz W,Trivedi R.Metall Trans,1991;22A:3051 [5]Li J F,Zhou Y H.Acta Mater,2005;53:2351 [6]Aziz M J.J Appl Phys,1982;53:1158 [7]Sobolev S L.Phys Rev,1997;55E:6845 [8]Wang H,Liu F,Chen Z,Yang G,Zhou Y.Acta Mater, 2007;55:497 [9]Wang H,Liu F,Yang W,Chen Z,Yang G,Zhou Y.Acta Mater,2008;56:746 [10]Goetzinger R,Barth M,Herlach D M.J Appl Phys,1998; 84:1643 [11]Li J F,Jie W Q,Zhao S,Zhou Y H.Metall Mater Trans, 2007;38A:1806 [12]Lipton J,Glicksman M E,Kurz W.Mater Sci Eng,1984; 65:57 [13]Trivedi R,Kurz W.Acta Metall,1986;34:1663 [14]Boettinger W J,Coriell S R,Trivedi R.In:Mehrabian R, Parrish P A,eds,,Rapid Solidification Processing:Prin- ciple and Technologies,Baton Rouge:Claitors,1987:13 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|