| TEXTURE EVOLUTION OF POLYCRYSTALLINE ALUMINUM FOR ROLLING DEFORMATION - II. Theoretical Simulation |
| Zhiyong Chen;;;; |
| 中南大学 |
|
Cite this article:
Zhiyong Chen. TEXTURE EVOLUTION OF POLYCRYSTALLINE ALUMINUM FOR ROLLING DEFORMATION - II. Theoretical Simulation. Acta Metall Sin, 2008, 44(11): 1322-1331 .
|
|
|
Abstract The rolling texture evolution with initial randomly distributed texture and nearly cube texture was simulated by Taylor-type models. A systematic comparison of the theoretical results obtained by the different type models against the experimental rolling textures is performed by orientation line analysis. The results shows that the orientation distribution calculated by the FC Taylor is closer to experimental results than those by other models at the low rolling deformation degree. During the higher deformation degrees, the results by the lath model agree the measured better for the initial randomly distributed texture while the simulated results obtained by the mixed are closer to the measured than those by the other models for initial cube texture.
|
|
Received: 28 February 2008
|
|
|
[1]Chen Z Y,Cai H N Chang Y Z,Zhang X M,Liu C M. Acta Metall Sin,2008;44:1316 (陈志永,才鸿年,常亚喆,张新明,刘楚明.金属学报,2008;44:1316) [2]Chen Z Y,Zhang X M,Zhou Z P,Li S Y,Yang Y.Trans Nonferrous Met Soc China,1999;9:307 [3]Taylor G I.J Inst Met,1938;62:307 [4]Mecking H.In:Nagashima S,ed.,Proc 6th Int Conf on Textures of Materials,Tokyo:Iron and Steel Institute of Japan,1981:53 [5]Bunge H J,Leffers T.Scr Metall,1971;5:143 [6]Canova G R,Kocks U F.In:Brakman C M,Jongenburger P,Mittemeijer E J,eds.,Proc 7th Int Conf on Textures of Materials,Noordwijkerhout:Netherlands Society of Ma- terials Science,1984:573 [7]Asaro R J,Needleman A.Acta Metall,1985,33:923 [8]Renouard M,Wintenberger M.C R Acad Sci,1976;283B: 237 [9]Honneff H,Mecking H.In:Gottstein G,L(?)cke K,eds., Proc 5th Int Conf on Textures of Materials,Aachen: Springer,1978:265 [10]van Houtte P.In:Nagashima S,ed.,Proc 6th Int Conf on Textures of Materials,Tokyo:Iron and Steel Institute of Japan,1981:428 [11]Kocks U F,Chandra H.Acta Metall,1982;30:695 [12]Fortunier R,Driver J H.Acta Metall,1987;35:509 [13]Hirsch J,L(?)cke K.Acta Metall,1988;36:2883 [14]Sachs E.Z Vet Deut Ing,1928;72:734 [15]Pérocheau F,Driver J H.Int J Plast,2000;16:73 [16]Raabe D,Zhao Z,Mao W.Acta Mater,2002;50:4379 [17]Cao P,Fang G,Lei L P,Zeng P.Acta Metall Sin,2007; 43:913 (曹鹏,方刚,雷丽萍,曾攀.金属学报,2007;43:913) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|