EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD
;
东北大学材料与冶金学院冶金物理化学研究所
Cite this article: 

;. EXPERIMENTAL RESEARCH OF PREPARATION OF CaB6 BY MOLTEN SALT ELECTROLYSIS METHOD. Acta Metall Sin, 2008, 44(10): 1243-1246 .

Download:  PDF(691KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The research is about synthesis process of CaB6 powder by molten salt electrolysis method. The synthesis temperature, electrolysis voltage, electrolysis time is identified. At the same time, under the conditions of different electrolysis time,the phase composition, particle size and shape of cathode products is analysised by X-ray diffraction and scanning electron microscope , experimental results show that synthesis process of CaB6 powder in CaCl2 molten salt system must have the basic conditions: protectiving environment of argon, electrolysis voltage is 3.0V, 900℃ insulation 30h, the range of CaB6 crystal particles size was 2μm~10μm, the morphology of particle is regular with rule cuboid massive crystal. The cathode electrolysis process conducted cyclic voltammetry scan analysis, a preliminary dynamic analysis and calculation to determine that chlorine borate proliferating to the cathode is control step of reaction.
Key words:  Molten salt electrolysis      Molten salt system      CaB6      Cyclic voltammetry      
Received:  22 January 2008     
ZTFLH:  TQ174.75  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I10/1243

[1]Yang L X,Min G H,Yu H S,Hart J D,Wang W T.J Chin Ceram Soc,2003;31:687 (杨丽霞,闵光辉,于化顺,韩建德,王维倜.硅酸盐学报,2003;31:687)
[2]Zheng S Q,Min G H,Zou Z D,Yu H S,Zhang C J.J Chin Ceram Soc,2001;29:128 (郑树起,闵光辉,邹增大,于化顺,张川江.硅酸盐学报,2001;29:128
[3]Dou Z H,Zhang T A,Hou C,Xu S X,Yang H,Li H.J Nonferrous Metals Soc,2004;14:322 (豆志河,张廷安,侯闯,徐淑香,杨欢,李皇.中国有色金属学报2004;14:322)
[4]Zheng S Q,Min G H,Zou Z D.J Am Ceram Soc,2001; 84:2725
[5]Shigek O.J Cryst Growth,1998;192:346
[6]Ma M,Wang D H,Wang W G.J Alloys Compd,2006; 420:37
[7]Chen Z,Fray D J,Farthing T W.Nature,2000;407:361
[8]Hu X F,Xu Q.Acta Metall Sin,2006;42:285 (胡小锋,许茜.金属学报,2006;42:285)
[9]Schwandt C,Fray D J.Electrochim Acta,2005;51:66
[10]Alexander D T L,Schwandt C,Fray D J.Acta Mater, 2006;54:2933
[11]Yu L P,Sun H J,He J,Wang D H,Jin X B,Hu X H, Chen G Z.Electrochem Commun,2007;9:1374
[12]Li G M,Wang D H,Jin X B,Chen G Z.Electrochem Commun,2007;9:1951
[13]Qiu G H,Wang D H,Jin X B,Chen G Z.Electrochim Acta,2006;5i:5785
[14]Zhang M L,Yan Y D,Hou ZY,Fan L A,Chen Z,Tang D X.J Alloys Compd,2007;440:362
[15]Allen J B,Larry R F(eds.),Shao Y H,Zhu G Y,Dong X D,Zhang B L(trans.).Electrochemical Methods Fun- damentals and Applications.Beijing:Chemical Industry Press,2005:160 (Allen J B,Larry R F著,邵元华,朱果逸,董献堆,张柏林译.电化学方法原理和应用.北京:化学工业出版社,2005:160)
[16]Bossuyt S,Madge S V,Chen G Z,Castellero A,Deledda S,Eckert J,Fray D J,Greer A L.Mater Sci Eng,2004; A375:240
[1] YANG Yulin, MU Zhangyan, FAN Zheng, DAN Zhenhua, WANG Ying, CHANG Hui. Nanoporous Silver via Electrochemical Dealloying and Its Superior Detection Sensitivity to Formaldehyde[J]. 金属学报, 2019, 55(10): 1302-1310.
[2] SONG Lixiao ZHANG Zhao ZHANG Jianqing CAO Chunan. ELECTROPLATING MECHANISM OF NANOSTRUCTURED BLACK Ni FILMS[J]. 金属学报, 2011, 47(1): 123-128.
[3] SHI Jinjie SUN Wei GENG Guoqing. INFLUENCE OF CARBONATION ON THE CORROSION PERFORMANCE OF STEEL HRB335 IN SIMULATED CONCRETE PORE SOLUTION[J]. 金属学报, 2011, 47(1): 17-24.
[4] ;. Investigation on Preparation of Tb2Fe17 by Direct Electrochemical Reduction of Tb4O7-Fe2O3 Pellet in Molten Calcium Chloride[J]. 金属学报, 2008, 44(7): 859-862 .
[5] YIN Renhe; ZHAO Yaping; DAI Yingchun; ZHANG Xinsheng. Effect of Sodium Salicylate on Electropolymerization of Pyrrole on Zincated Steel[J]. 金属学报, 2004, 40(2): 168-172 .
[6] DU Senlin;SU Mingzhong;Changchun Institute of Applied Chemistry; Academia Sinica. ELECTROCHEMICAL BEHAVIOUR OF Nd~3+ REDUCED ON LIQUID Ga ELECTRODE IN MOLTEN CHLORIDE[J]. 金属学报, 1991, 27(3): 111-115.
[7] YAN Licheng;YANG Jinxiu;ZHU Lei;XU Jingyan;FAN Jinxia Shanghai University of Science and Technology Suzhou Teachers' School Department of Chemistry;Shanghai University of Science and Technology; Shanghai 2018000. PHASE DIAGRAMS OF KF-LiCl-BaCl_2 AND LiF-LiCl-BaCl_2 SYSTEMS[J]. 金属学报, 1990, 26(2): 142-145.
No Suggested Reading articles found!