Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (10): 1198-1202     DOI:
Research Articles Current Issue | Archive | Adv Search |
Modeling of Three-Phase Flows and Slag Layer Behavior in an Argon Gas Stirred Ladle
东北大学材料与冶金学院
Cite this article: 

. Modeling of Three-Phase Flows and Slag Layer Behavior in an Argon Gas Stirred Ladle. Acta Metall Sin, 2008, 44(10): 1198-1202 .

Download:  PDF(1962KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A Mathematical model has been developed to analyze the transient three- dimensional and three–phase flow in an argon gas bottom stirring ladle with one porous plugs. Multiphase Volume of Fluid (VOF) method is used to simulate the slag layer behaviors. Numerical results produce the following transient phenomena: when argon gas is injected into molten steel in a ladle, gas rising passage is formed near the plug, and then bubbles are created in the interior of molten steel; the rising gas bubbles impinge the slag intermittently and breakthrough the slag layer to create the slag eye. Simultaneity, the wave at interface of slag-steel formed and wave frequency increases with the increasing of argon gas flow rate for one off-centered plug case. Parametric studies show that diameter of slag eye changes from 0.43 m to 0.81 m while the argon gas flow rate vary with 100 ~300 Nl/min for a 220 ton ladle. The non-dimensional areas of slag eye vs the modified Froude number is close to experimental data in literature. Significant deformation of slag layer occurs during gas stirring operation, the thickness of slag becomes thin near the slag eye and thick near the ladle wall accordingly. The steel downward flow velocity at the slag eye periphery can be affected significantly by Ar gas flow rate. The higher the velocity, the more slag emulsification can be expected.
Key words:  Ladle metallurgy      Slag layer behavior      Three-phase flow      Mathematical model      
Received:  25 March 2008     
ZTFLH:  TF769.9  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I10/1198

[1]Ridenour P,Yin H B,Balajee S R,Chaubal P,Zhou Q. In:Ashburn R E ed.,AIS Tech 2006-Proceedings of the Iron and Steel Technology Conference,Cleveland,Ohio, 2006:721
[2]Beskow K,Dayal P,Bjorkvall J,Nzotta M,Sichen D.Iron- mak Steelmak,2006;33:74
[3]Lachmund H,Xie Y K,Buhles T,PluschketI W.Steel Res Int,2003;74:77
[4]Han J W,Heo S H,Kam D H,You B D,Park J J,Song H S.ISIJ Int,2001;41:1165
[5]Jonsson L,Sichen D,J(?)nsson P.ISIJ Int,1998;38:260
[6]Krishnapisharody K,Irons G A.Metall Mater Trans,2006; 37B:763
[7]Yonezawa K,Schwerdtfeger K.Metall Mater Trans,1999; 30B:411
[8]Jonsson L,Jonsson P.ISIJ Int,1996;36:1127
[9]Hirt C W,Nichols B D.J Comput Phys,1981;39:201
[10]Li B K,He J C,Lu Z W.Acta Metall Sin,1993;29:143 (李宝宽,赫冀成,陆钟武.金属学报,1993;29:143)
[11]Mazumdar D,Guthrie R I L.ISIJ Int,1995;35:1
[12]Mazumdar D,Guthrie R I L.Metall Trans,1995;25B:3085
[1] Dunming LIAO, Liu CAO, Fei SUN, Tao CHEN. Research Status and Prospect on Numerical Simulation Technology of Casting Macroscopic Process[J]. 金属学报, 2018, 54(2): 161-173.
[2] Xuewei YAN,Ning TANG,Xiaofu LIU,Guoyan SHUI,Qingyan XU,Baicheng LIU. MODELING AND SIMULATION OF DIRECTIONAL SOLIDIFICATION BY LMC PROCESS FOR NICKEL BASE SUPERALLOY CASTING[J]. 金属学报, 2015, 51(10): 1288-1296.
[3] XiaoGuang Zhou. Modelling of Dynamic Recrystallization for Nb Bearing Steels on Flexible Thin Slab Rolling[J]. 金属学报, 2008, 44(10): 1188-1192 .
[4] LI Weibiao; WANG Fang; QI Fengsheng; LI Baokuan. Mathematical Model on Steel Strip--Feeding of Mold in Continuous Casting Process[J]. 金属学报, 2007, 43(11): 1191-1194 .
[5] . A NEW MATHEMATICAL MODEL FOR HARDENABILITY OF STEELS[J]. 金属学报, 2006, 42(3): 265-272 .
[6] . MATHEMATICAL MODEL OF U-CURVE OF STEELS[J]. 金属学报, 2006, 42(10): 1019-1024 .
[7] XU Daming ; ZHANG Chengjun ; SI Guangju (School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001)(Engineering College; Jiamusi University; Jiamusi 154007). MICRO-/MACRO-SCOPIC MODELING OF SOLUTAL MASS TRANSPORT IN DENDRITE SOLIDIFICAfION WITH PARTIAL SOLID BACK DIFFUSION[J]. 金属学报, 1998, 34(7): 678-688.
[8] GUAN Kezhi; FAN Bailin; ZHOU Jihua(University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1995-10-30; in revised form 1996-03-26). FLOW STRESS OF BRASS AT HOT DEFORMATION[J]. 金属学报, 1996, 32(7): 749-754.
[9] SHENG Dongyuan; NI Mansen; DENG Kaiwen; LIU Jiaqi; GAN Yong; XIAO Zeqiang (National Research & Engineering Center of Continuous Casting Technology;Gentral Iron and Steel Research Institute; Ministry of Metallurgical industry;Beijing 100081)(Manuscript received 1995-11-09; in revised form 1996-04-17). MATHEMATICAL MODEL OF FLUID FLOW,TEMPERATURE CONTROL AND INCLUSION BEHAVIOUR IN CONTINUOUS CASTING TUNDISH[J]. 金属学报, 1996, 32(7): 742-748.
[10] HUANG Dianbing; YANG Xuemin; YANG Tianjun; KONG Lingtan (University of Science and Technology Beijing; Beijing 100083). KINETICS AND MATHEMATICAL MODEL FOR REDUCTION PROCESS OF IRON ORE BRIQUETTE CONTAINING CARBON[J]. 金属学报, 1996, 32(6): 629-636.
[11] YIN Aijun; LI Jing; LI Hinhai; HUANG Kexiong; JIANG Hanying (Central South University of Technology; Changsha 410083) (Manuscript received 1995-06-30; in revised form 1995-12-01). COMPUTER SIMULATION ON MINOR ELEMENT BEHAVIOUR IN COPPER FLASH SMELTING[J]. 金属学报, 1996, 32(4): 387-392.
[12] LI Baowei; HE Youduo(Baotou institute of Iron and Steel;Baotou 014010);Y. SAHAI(The Ohio State University; USA)(Manuscript received 1995-05-30). A MATHEMATICAL MODEL OF POST-COMBUSTION AT THE INITIAL STAGE IN TOP-BLOWN CONVERTER[J]. 金属学报, 1996, 32(2): 169-174.
[13] ZHU Miaoyong; (Department of Ferrous Metallurgy; Northeastern University;Shenyang 110006) INOMOTO Takeo; XIAO Zeqiang(Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Futtsu; Japan). MATHEMATICAL AND PHYSICAL MODELING OF FLOW AND MIXING IN LADLES STIRRED BY ARGON THROUGH MULTI-TUYERE[J]. 金属学报, 1995, 31(22): 435-439.
[14] ZHU Miaoyong; SW ADA Ikuo; XIAO Zeqiang (Northeastern University; Shenyang 110006)(Nippon Steel Corporation; Kawasaki 211 Japan)(Manuscript received 1994-03-30; in revised form. 1995-03-13). PHENOMENA OF THREE-DIMENSIONAL FLOW AND MIXING IN ARGON-STIRRED LADLES[J]. 金属学报, 1995, 31(20): 346-352.
[15] cLI Baowei; HE Youduo(Baotou Univevsity of Iron Steel Technology; Baotou 014010);SAHAI Y(Ohio Staie Universily; U.S.A.)(Manuscript received 1994-05-30; in revised form 1994-12-19). A MATHEMATICAL MODEL OF DROPLET GENERATION, MOVEMENT AND HEAT TRANSFER IN BOF[J]. 金属学报, 1995, 31(16): 145-151.