Abstract The crystal structure and magnetic properties of non-stoichiometric MnFe(P,Si,Ge) alloys have been investigated by X-ray powder diffraction and magnetic measurements. XRD analysis indicates that all the samples consist of the hexagonal Fe2P-type structure phase mainly and a small amount of the second phase Fe2MnSi. The superfluous of Mn and Fe can reduce the Curie temperature which from 343K to 294K (superfluous Mn) and 286K (superfluous Fe). The superfluous of Fe can decrease the thermal hysteresis, but the superfluous of Mn can increase it. However, the entropy change as well decreased from 5.2 J•kg-1•K-1 (stoichiometric) to 4.9 J•kg-1•K-1 (superfluous Mn) and 3.8 J•kg-1•K-1 (superfluous Fe).
|
|
Received: 22 November 2006
|
|
|
[1]Tegus O,Brück E,Buschow K H J,de Boer F R.Nature, 2002;415:150 [2]Pecharsky V K,Gschneidner J K A.Phys Rev Lett,1997; 78:4494 [3]Brück E,Tegus O,Zhang L,Li X W,de Boer F R, Buschow K H J.J Alloys Compd,2004;383:32 [4]Tegus O,Fuquan B,Dagula W,Zhang L,Brück E,Si P Z,de Boer F R,Buschow K H J.J Alloys Compd,2005; 396:6 [5]Dagula W,Tegus O,Li X W,Song L,Brück E,Cam Thanh D T,de Boer F R,Buschow K H J.J Appl Phys, 2006;99:08Q105 [6]Brück E,Ilyn M,Tishin A M,Tegus O.J Magn Magn Mater,2005;290-291:8 [7]Tegus O,Brück E,Li X W,Zhang L,Dagula W,de Boer E R,Buschow K H J.J Magn Magn Mater,2004;272-2?6: 2389 [8]Tegus O,Brück E,Zhang L,Dagula W,Buschow K H J, de Boer F R.Physica,2002;319B:174 [9]Brück E,Tegus O,Li X W,de Boer F R,Buschow K H J.Physic.a,2003;327B:431 [10]Zener C.Phys Rev,1951;82:403 [11]Millis A J,Littlewood P B,Shraiman B I.Phys Rev Lett, 1995;74:5144 [12]Zhang L.PhD Dissertation,University of Amsterdam, 2005 [13]Bacmann M,Soubeyroux J L,Barrett R.J Magn Magn Mater,1994;134:59 [14]McGuire T R,Gupta A,Duncombe P R.J Appl Phys, 1996;79:4549 [15]Dionne G F.J Appl Phys,1996;79:172% |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|