Abstract  We present ab initio calculations of the thermal properties of hcp metals Zr. We show that the thermal properties such as thermal expansions and heat capacities in hcp metal can be calculated precisely within the quasiharmonic approximation, by using phonon dispersions from density-functional perturbation theory, and the pseudopotential plane-wave method. Our results for the thermal properties are in good agreement with available experimental data in a wide range of temperatures.
Key words:       
Received:  20 December 2006     
ZTFLH:  TG335  
  TB159  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I8/883

[1]Courtney T H.Mechanical Behaviour of Materials.2nd ed.,New York:McGraw-Hill,2000:182
[2]Sanders P G,Eastman J A,Weertman J R.Acta Mater. 1997;45:4019
[3]Zhao J H,Chen Q Y.Acta Metall Sin,2002;38:166 (赵继华,陈启元.金属学报,2002;38:166)
[4]Feng R,Li H M.Sonochemistry and Its Applications. Hefei:Anhui Science & Technology Press,1992:67 (冯若,李化茂.声化学及其应用.合肥:安徽科技出版社,1992:67)
[5]Suslick K S.Science,1990;247:1439
[6]Senapati N.Adv Sonochem,1991;2:187
[7]Vasudevan R,Devanathan R.Met Finish,1992;90:23
[8]Prasad P,Ahila S,Vasudevan R,Seshadri S K.Indian J Chem Technol,1994;1:127
[9]Prasad P,Vasudavan R,Seshadri S K.J Mater Sci Lett, 1992;11:1424
[10]Prasad P,Vasudevan R,Seshadri S K.J Mater Sci Lett, 1993;12:902
[11]Prasad P,Ahila S,Vasudavan R,Seshadri S K.J Mater Sci Lett,1994;13:15
[12]Zhu J J,Aruna S T,Yuri K.Chem Mater,2000;12:143
[13]Shen Y F,Lu L,Lu Q H,Jin Z H,Lu K.Scr Mater,2005; 52:989
[14]Robertson A,Erb U,Palumbo G.Nanostruct Mater,1999; 12:1035
[15]Jia N,Wang Y D,Wu S D,Han W Z,Wang Y N,Deng J N,Liaw P K.Scr Mater,2006;54:1247
[16]Knapp J A,Follstaedt D M.J Mater Res,2004;19:218
[17]Siegel R W,Fougere G E.Nanostruct Mater,1995;6:205
[18]Nieh T G,Wadsworth J.Scr Metall Mater,1991;25:955
[19]Mitra R,Hoffman R A,Madan A,Weertman J R.J Mater Res,2001;16:1010
[20]EI-Sherik A M,Erb U,Palumbo G,Aust K T.Scr Metall Mater,1992;27:1185
[21]Dalla Torre F,Van Swygenhoven H,Victoria M.Acta Mater,2002;50:3957
[22]Liu C P.Physical Chemistry of Cu Hydrometallurgy.Bei- jing:Chinese Science & Technology Press,1991 (刘纯鹏.铜的湿法冶金物理化学.北京:中国科学技术出版社,1991)
[23]Li Y G,Chrzanowski W,Lasia A.J Appl Electrochem, 1996;26:843
[24]Gonzalez-Garcia J,Saez V,Iniesta J S,Montiel V,Aldaz A.Electrochem Commun,2002;4:370
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!