| Cathodic Electro—Deposition of WO3 And Its Photoelectrochemical Anticorrosion for Copper Under Visible Light |
| LENG Wenhua; LIU Dongpo;CHENG Xiaofang; ZHU Wencai;ZHANG Jianqing;CAO Chunan |
| Chemistry Department; Zhejiang University |
|
Cite this article:
LENG Wenhua; LIU Dongpo; CHENG Xiaofang; ZHU Wencai; ZHANG Jianqing; CAO Chunan. Cathodic Electro—Deposition of WO3 And Its Photoelectrochemical Anticorrosion for Copper Under Visible Light. Acta Metall Sin, 2007, 43(7): 764-768 .
|
|
|
|
|
Received: 23 November 2006
|
|
|
[1]Wu P F,Li M C,Shen J N,Xiao M Q,Liu D.Corros Sci Prote Technol,2005;17:104 (武朋飞,李谋成,沈嘉年,削美群,刘东,腐蚀科学与防护技术,2005;17:104 [2]Zhang J Q,Leng W H,Cheng X F,Liu D P.J Chin Soc Corros Prote,2006;26:188 (张鉴清,冷文华,程小芳,刘东坡,中国腐蚀与防护学报,2006; 26:188) [3]Ohko Y,Saitoh S,Tatsuma T,Fujishima A.J Electrochem Soc,2001;148:B24 [4]Ohko Y,Saitoh S,Tatsuma T,Fujishima A.Electrochem Solid State Lett,2002;5(2):B9 [5]Huang J,Shinohara T,Tsujikawa S.Zairyo Kankyo,1997; 46:651 (Huang J,Shinohara T,Tsujikawa S.材料环境,1997; 46:651) [6]Hyunwoong P,Kyoo-Young K,Wonyong C.J Phys Chem, 2002;106 B:4775 [7]Yuan J,Tsujikawa S.J Electrochem Soc,1995;142:3444 [8]Subasri R,Shimohara T,Mori K.J Electrochem Soc,2005; 152:B105 [9]Subasri R,Shimohara T.Electrochem Solid State Lett, 2004;7(7):B17 [10]Subasri R,Shimohara T.Electrochem Commun,2003;5: 897 [11]Fujisaws R,Tsujikawa S.Mater Sci Forum,1995;185- 188:1075 [12]Yuan J,Tsujikawa S.Zairyo Kankyo,1995;44:534 (Yuan J,Tsujikawa S.材料环境,1995;44:534) [13]Huang J,Shinohara T,Tsujikawa S.Zairyo Kankyo,1999; 48:575 (Huang J,Shinohara T,Tsujikawa S.材料环境,1999; 48:575) [14]Li M C,Suzhen L,Pengfei W,Jianian S.Electrochim Acta, 2005;50:3401 [15]Tatsuma T,Saitoh S,Ohko Y,Fujishima A.Chem Mater, 2001;13:2838 [16]Solarska R,Santato C,Jorand-Sartoretti C.J Appl Elec- trochem,2005;35:715 [17]Shi J Y,Leng W H,Cheng X F,Zhang J Q,Cao C N. Acta Phys Chinm Sin,2005;21:971 (施晶莹,冷文华,程小芳,张鉴清,曹楚南.物理化学学报, 2005;21:971) [18]Zhu W C.Master Thesis.Zhejiang University,Hangzhou, 2006 (朱文彩.浙江大学硕士学位论文.杭州,2006) [19]The Research Group of Analytic Method for Environmen- tal Pollution.Analytic Method for Environmental Pollu- tion(Vol.1:Analysis of Inorganic Compound).2nd Edi- tion,Beijing:Science Press,1987 (环境污染分析方法科研协作组.环境污染分析方法(第一卷,无机物分析).北京:科学出版社,1987) [20]Santato C,Odziemkowski M,Ulmann M,Augustynski J. J Am Chem Soc,2001;123:10639 [21]Hoffmann M R,Martin S T,Choi W,Bahnemann D W. Chem Rev,1995;95:69 [22]Leng W H,Zhang Z,Zhang J Q,Cao C N.J Phys Chem, 2005;109B:15008 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|