Study of Interfaces in SiC Fiber Reinforced Nickel-Based Composites
;;;;
东北大学
Cite this article: 

. Study of Interfaces in SiC Fiber Reinforced Nickel-Based Composites. Acta Metall Sin, 2007, 43(4): 444-448 .

Download:  PDF(456KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Interface reaction between SiC fiber and matrix is a major problem which directly influences the mechanical properties. In this article, the SiO2-Al2O3,C-Al2O3 layers have been coated on the surface of the SiC fibers as the barrier layer to inhibit the SiCf/Ni element mutual diffusion. The SiCf/Ni composites have been prepared by vacuum heat press. The coatings can effectively block the SiCf/Ni element mutual diffusion and protect fiber’s integration well after heat treatment in vacuum at 850-950℃ for150 hours. The SEM observation indicated that a compact Al2O3 layer is well coated on the surface of the fiber. In contrast, the SiO2 coating is weakness and brittleness combine with fiber, and some cracks in the interface can be seen clearly. The C layer in the C-Al2O3 coating disappeared and dissolved after heat treatment at 850-950℃ for 100 hours.
Key words:       
Received:  27 June 2006     
ZTFLH:  TG146.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I4/444

[1]Mileiko S T,Kiiko V M,Kolchin A A,Serebryakov A V, Korzhov V P,Starostin M Y,Sarkissyan N S.Compos Sci Technol,2002;62:167
[2]Mileiko S T,Kiiko V M,Kolchin A A,Korzhov V P, Prokopenko V M.Corapos Sci Technol,2002;62:181
[3]Mileiko S T.Compos Sci Technol,2002;62:195
[4]Hu W,Karduck P,Gottstein G.Acta Mater,1997;45: 4535
[5]Zhang W,Smith J R,Evans A G.Acta Mater,2002;50: 3803
[6]Yu Q,Chen P,Lu C.Insulant Mater,2005;2:50 (于祺,陈平,陆春.绝缘材料,2005;2:50)
[7]Cai S,Li Z Y,Dang Y,Yan M G.J Aeronaut Mater,2006; 26(2):22 (蔡杉,李占一,董妍,颜鸣皋.航空材料学报,2006; 26(2):22)
[8]Feng C X,Xue J G,Song Y C.Hi-Tech Fiber Appl,2003; 28(1):15 (冯春祥,薛金根,宋永才.高科技纤维与应用,2003;28(1): 15)
[9]Yu Y X,Cao F,Li X D.Acta Mater Compos Sin,2004; 21(5):79 (余煜玺,曹峰,李效东.复合材料学报,2004;21(5):79)
[10]Tang W M,Zheng Z X,Ding H F,Jin Z H.J Chin Ceram Soc,2003;31:287 (汤文明,郑治祥,丁厚福,金志浩.硅酸盐学报,2003;31: 287)
[11]Li R J.Creramic-Metal Composite.Beijing:Metallurgical Industry Press,2004,99 (李荣久.陶瓷-金属复合材料.北京:冶金工业出版社,2004, 99)
[12]Mittncki M A:SAMPE,1990;26(5):49
[13]Feng Z D,He L Z,Wang Y Y.Phys Chem Insp-Phys Fasc,2005;41(Suppl.):59 (冯祖德,何立志,王艳艳.理化检验-物理分册,2005;41(增刊):59)
[14]Zheng C M,Li X D,Wang Y F,Wang Y D,Feng C X. Aerosp Mater Technol,2005;35(3):7 (郑春满,李效东,王亦菲,王应德,冯春祥.字航材料工艺, 2005;35(3):7)
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!