STUDIES OF Nb–TiAl ALLOY BY POSITRON ANNIHILATION TECHNIQUES
ZHANG Lanzhi; WANG Baoyi;WANG Danni; WEI Long; LIN Junpin;WANG Wenjun
Key Laboratory of Nuclear Analysis Techniques; Institute of High Energy Physics; Chinese Academy of Sciences; Beijing 100049
Cite this article: 

ZHANG Lanzhi; WANG Baoyi; WANG Danni; WEI Long; LIN Junpin; WANG Wenjun. STUDIES OF Nb–TiAl ALLOY BY POSITRON ANNIHILATION TECHNIQUES. Acta Metall Sin, 2007, 43(3): 269-272 .

Download:  PDF(696KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Positron annihilation lifetime and coincidence Doppler broadening measurements have been performed in Ti51Al49 alloy with different amounts of Nb doped. The experimental results indicate that when a low mount of Nb atoms is added into Ti51Al49 alloy, the Nb atoms mainly aggregate at grain boundaries, and then the free electron density increases, which reduces the brittleness of TiAl alloys. In contrast, the density of free electron in grain boundaries and in bulk are both decrease in high Nb doped alloy, due to the formation of the new order structure, which increases the brittleness of TiAl alloys.
Key words:  positron annihilation lifetime      coincidence Doppler broadening      
Received:  10 August 2006     
ZTFLH:  TG146.2  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V43/I3/269

[1]Viswanathan G B,Vasudevan V K,Mills M J.Acta Mater, 1999;47:1399
[2]Kim Y W.Mater Sci Eng,1995;A192/193:519
[3]Dimiduk D M.Mater Sci Eng,1999;A263:281
[4]Chen G L,Sun Z Q,Zhou X.Mater Sci Eng,1992;A153: 597
[5]Déve H E,Evans A G,Odette G R,Mehrabian R,Emiliani M L,Hecht R J.Acta Metall Mater,1990;38:1491
[6]Kim Y W.JOM,1989;41(7):24
[7]Asoka-Kumar P,Alatalo M,Ghosh V J,Kruseman A C, Nielsen B,Lynn K G.Phys Rev Lett,1996;77:2097
[8]Nagai Y,Hasegawa M,Tang Z,Hempel A,Yubuta K, Shimamura T,Kawazoe Y,Kawai A,Kano F.Phys Rev, 2000;61B:6574
[9]Nagai y,Tang Z,Hasegawa M,Kanai T,Saneyasu M. Phys Rev,2001;63B:134110
[10]Onitsuka T,Takenaka M,Kuramoto Y,Nagai Y, ??Hasegawa M.Phys Rev,2001;65B:012204
[11]Deng W,Huang Y Y,Brusa R S.J Alloy Compd,in press
[12]Somoza A,Petkov M P,Lynn K G.Phys Rev,2002;65B: 094107
[13]Wang B Y,Wang T M.J Lanzhou Univ,1992;28(3):55 (王宝义,王天民.兰州大学学报,1992;28(3):55)
[14]Brandt W,Paulin R.Phys Rev,1972;5B:2430
[15]Brandt W,Reinheime J.Phys Rev,1970;2B:3104
[16]Morinaga M,Saito J,Yukawa N,Adachi H.Acta Metall Mater,1990;38:25
[17]Zhong X P,Deng W,Tang Y S,Xiong L Y,Wang S H, Gou J T,Long Q W.Acta Phys Sin,1998;47:1734 (钟夏平,邓文,唐郁生,熊良钺,王淑荷,郭建亭,龙期威.物理学报,1998;47:1734)
[18]Deng W,Huang Y Y,Wu D H,Cao M Z,Xiong L Y. Mater Lett,2002;56:593
[19]Brandt W,Dupasquier A.Positron Solid-State Physics. New York:Amsterdam,1983:200
[20]Huang Y Y,Wu W M,Deng W,Zhong X P,Xiong L Y, Cao M Z,Long Q W.Chin J Nonferrous Met,2000;10: 796 (黄宇阳,吴伟明,邓文,钟夏平,熊良钺,曹名洲,龙期威.中国有色金属学报,2000;10:796)
[21]Chen G L,Zhang L C,Zhang W J.Intermetallics,1999; 7:1211
[22]Lei X Y,Yah W Q,Liang Q H.Heat Treat Met,2001;2: 11 (雷新颖,闫蕴琪,梁清华.金属热处理,2001;(2):11)
[23]Greenberg B A,Antonava O V,Indenbaum V N,Karkina L E,Notkin A B,Ponomarev M V,Smirnov L V.Acta Metall Mater,1991;39:233
[1] GAO Yingjun; WU Weiming; FENG Guanzhi; XU Shaojie; RUAN Xiangdong(Guangxi University; Nanning 530004)(Manuscript received 94-03-11). POSITRON ANNIHILATION LIFETIME ANALYSIS OF 8090 ALLOY WITH DOPING Zn, Ag OR Sc UNDER CRYOGENIC TEMPERATURES[J]. 金属学报, 1995, 31(14): 91-96.
No Suggested Reading articles found!