| ELECTROPOLYMERIZATION AND RADIATION CROSSLINKING OF ANTICORROSION POLYANILINE FILMS ON ZINC-ELECTROPLATED STEEL |
| YIN Renhe; JI Xuebin; WANG Huijuan; ZHANG Lei; SHI Xinhong |
| Department of Chemistry; College of Science; Shanghai University; Shanghai 200444 |
|
Cite this article:
YIN Renhe; JI Xuebin; WANG Huijuan; ZHANG Lei; SHI Xinhong. ELECTROPOLYMERIZATION AND RADIATION CROSSLINKING OF ANTICORROSION POLYANILINE FILMS ON ZINC-ELECTROPLATED STEEL. Acta Metall Sin, 2007, 43(3): 273-280 .
|
|
|
Abstract Polyaniline films were synthesized on zinc-electroplated steel sheets in sodium salicylate aqueous medium.From the FTIR and XPS values, conclusions can be as follows: (1) Pani layers is doped with some salicylate anions; (2) The doping level is nearly 12~24% for the Pani films.A research is made on the effect of the radialization of electron beam on electropolymerized film of aniline film on zinc-electroplated steel. The obtained results show that the gel content and crosslinking density increase with the dose, get to a maximum at 960kGy, and are independent of dosage quotiety. The corrosion protection capability are improved to a great extent. At the same dose, the corrosion protection capability becomes better with the dosage quotiety becomes lower.
|
|
Received: 27 June 2006
|
|
|
[1]Zhao Y P,Yin R H,Cao W M,Yuan A B.Acta Metall Sin(Engl Lett),2004;17:849 [2]Zhang D H,Wang Y Y,Qiang J F.New Chem Mater, 2003;31(6):30 (张东华,王杨勇,强军锋.化工新型材料.2003;31(6):30) [3]Zhang H L.Guangxi Chem Ind,1998;27(3):37 (郑海林.广西化工,1998;27(3):37) [4]Nguyen Thile H,Carcia B,Deslouis C,Le X Q.Elec- trochem Acta,2001;46:4259 [5]Ha H F,Wu J L.Radialization Chemistry of Macromolecule-Principle and Application.Beijing: ??Peking University Press,2002:75 (哈鸿飞,吴季兰.高分子辐射化学——原理与应用.北京:北京大学出版社,2002:75) [6]Zhang Z C,Ge X W,Zhang M W.Radialization Chem- istry of Macromolecule.Hefei:University of Science and Technology of China Press,2002:106 (张志成,葛学武,张曼维.高分子辐射化学.合肥:中国科学技术大学出版社,2000:106) [7]Jing X L,Zhao W B,Zheng M S.Petrochem Technol Appl, 2001;19:225 (井新利,赵卫兵,郑茂盛.石化技术与应用,2001;19:225) [8]Sun J P,Li B M,Wu H C.Fine Chem,2002;19:578 (孙建平,李宝铭,吴洪才.精细化工,2002;19:578) [9]Zhang B Y,Gao Z,Su X M.Petrochem Technol Appl, 2005;23:11 (张柏宇,高治,苏小明.石化技术与应用.2005;23:11) [10]Camalet J L,Lacroix J C,Nguyen T D,Aeiyach S,Pham M C,Petitjean J,Lacaze P C.J Electroanal Chem,2000; 485(1):13 [11]Liu C M,Qiu J J,Tian D T.J Microwaves,2002;18:83 (刘承美,邱进俊,田大听.微波学报,2002;18:83) [12]Yuan A B,Xu N X.Battery,2002;32:323 (袁安保,徐乃欣.电池,2002;32:323)w |