| INFLUENCE OF La DOPING ON THE STRUCTURE,MAGNETIC AND ELECTRICAL TRANSPORT PROPERTIES OF Pr0.75Na0.25MnO3 |
| ZHANG Xinghua; LI Zhiqing; JIANG Enyong |
| 天津大学理学院应用物理系 |
|
Cite this article:
ZHANG Xinghua; LI Zhiqing; JIANG Enyong. INFLUENCE OF La DOPING ON THE STRUCTURE,MAGNETIC AND ELECTRICAL TRANSPORT PROPERTIES OF Pr0.75Na0.25MnO3. Acta Metall Sin, 2006, 42(9): 974-978 .
|
|
|
Abstract Polycrystalline (Pr 1-x La x)0.75Na0.25MnO3 (0.00≤x≤1.00) manganites were prepared by sol-gel method. X-ray Diffraction patterns showed that the samples are crystallized in single phase with perovskite-like structure. The structure of the compounds transforms from orthorhombic structure for x≤0.50 to rhombohedral structure for x≥0.70. The introduction of La3+ ions also suppresses the charge ordering in the samples. The charge ordering transition temperature decreases with increasing La3+ doping when x≤0.10. The charge ordering phenomenon disappeared for the samples with x>0.10, paramagnetic-ferromagnetic transition appeared, while the insulator-metal transition can be observed. For x≥0.50, the compounds also show large magnetic entropy change under low field near or above room temperature, indicating the material can be used in magnetic refrigeration.
|
|
Received: 08 December 2005
|
|
|
[1]Helmolt R V,Wecker J,Holzapfel B,Schultz L,Samwer K.Phys Rev Lett,1993;71:2331 [2]Jin S,Tiefel T H,McCormack M,Fastnacht R A,Ramesh R,Chen L H.Science,1994;264:413 [3]Wollan E O,Koehler W C.Phys Rev,1955;100:545 [4]Jirák Z,Krupi(?)ka S,(?)in(?)a Z,DlouáM,Vratislav S.J Magn Magn Mater,1985;53:153 [5]Uehara M,Mori S,Chen C H,Cheong S-W.Nature,1999;399:560 [6]F(?)th M,Freisem S,Menovsky A A,Tomioka Y,Aarts J,Mydosh J A.Science,1999;285:1540 [7]Guo Z B,Zhang J R,Huang H,Ding W P,Du Y W.Appl Phys Lett,1996;70:904 [8]Guo Z B,Du Y W,Zhu J S,Huang H,Ding W P,Feng D.Phys Rev Lett,1997;78:1142 [9]Bohigas X,Tejada J,del Barco E,Zhang X X,Sales M.Appl Phys Lett,1998;73:390 [10]Tomioka Y,Okuda T,Okimoto Y,Asamitsu A,Kuwahara H,Tokura Y.J Alloy Compd,2001;326:27 [11]Rao C N R,Arulraj A,Cheetham A K,Raveau B.J Phys:Condens Matter,2000;12:R83 [12]Hejtmanek J,Jirák Z,Sebek J,Strejc A,Hervieu M.J Appl Phys,2001;89:7413 [13]Li Z Q,Zhang X H,Liu H,Liu X J,Liu X D,Mi W B,Bai H L,Jing X N,Jiang E Y.Solid State Commun,2004;130:563 [14]Roy S,Guo Y Q,Venkatesh S,All N.J Phys:Condens Matter,2001;13:9547 [15]Zhong W,Chen W,Ding W P,Zhang N,Hu A,Du Y W,Yan Q J.J Magn Magn Mater,1999;195:112 [16]Zhong W,Chen W,Ding W P,Zhang N,Du Y W,Yan Q J.Solid State Commun,1998;106:55 [17]Li Z Q,Jiang E Y,Zhang D X,Hou D L,Li W C,Bai H L.Phys Lett,2000;277A:56 [18]Young R A,Sakthivel A,Moss T S,Paiva-Aantos C O.J Appl Cryst,1995;28:366 [19]Zhang X H,Li Z Q,Song W,Du X W,Wu P,Bai H L,Jiang E Y.Solid State Commun,2005;135:356 [20]Li Z Q,Zhang X H,Yu J S,Liu X J,Liu X D,Liu H,Wu P,Bai H L,Sun C Q.Lin J J,Jiang E Y.Phys Lett,2004;325A:430 [21]Rao G H,Sun J R,B(?)rner K,Hamad N.J Phys:Condens Matter,1999;11:1523 [22]Damay F,Martin C,Maignan A,Raveau B.J Appl Phys, 1997;82:6181 [23]Yu M H,Devi P S,Lewis L H,Sampath S,Parise J B, Gambino R J,Mater Sci Eng,2003;B97:245 [24]Phan M H,Tian S B,Yu S C,Ulyanov A N.J Magn Magn Mater,2003;256:306 [25]Ju H L,Gopalakrishnan J,Peng J L,Li Q,Xiong G C, Wenkatesan T,Greene R L.Phys Rev,1995;51B:6143 [26]Radaelli P G,Cox D E,Marezio M,Cheong S-W,Schiffer P E,Kamirez A P.Phys Rev Lett,1995;75:4488 [27]Phan M H,Peng H X,Yu S C,Tho N D,Chau N.J Magn Magn Mater,2005;285:199 [28]Sun Y,Tong W,Zhang Y H.J Magn Magn Mater,2001;232:205 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|