| Experimental Simulation of N--EMBr on Strip Casting with Twin Roll |
| LI Qisheng; DENG Kang; LEI Zuosheng; LI Weixuan; REN Zhongming |
| Shanghai Enhanced Laboratory of Ferro--Metallurgy; Shanghai University; Shanghai 200072 |
|
Cite this article:
LI Qisheng; DENG Kang; LEI Zuosheng; LI Weixuan; REN Zhongming. Experimental Simulation of N--EMBr on Strip Casting with Twin Roll. Acta Metall Sin, 2006, 42(7): 751-756 .
|
|
|
Abstract A model for simulating suppression of level fluctuation in mold of twin-roll strip caster with nozzle electromagnetic brake (N-EMBr), which imposed stationary magnetic field and direct current in nozzle, was established. Momentum of metal liquid in nozzle and level fluctuation in twin-roll pool were measured under different conditions, including immerging depth of nozzle, current and magnetic field. The experiment results showed that momentum of liquid metal, amplitude and frequency of fluctuation all were decreased with current increasing. It was found that N-EMBr technique for fluctuation suppression is effective to twin-roll strip casting mold.
|
|
Received: 21 October 2005
|
|
|
[1] Li B Q.JOM,1995;47(5): 29 [2] Zapuskalov N. ISIJ Int, 2003, 43: 1115 [3] Wang X D.Master's Degree Thesis,Shanghai University, Shanghai,2004 (王晓东,上海大学硕士学位论文,上海, 2004) [4] Guthrie R I. L, Isac M. Steel Res,1999; 70: 343 [5] Kim D S,Kim W S,Kuznetsov A V.Numerical Heat Transfer, 2002; 41A: 1 [6] Seyedein S H,Hasan M. Numer Heat Transfer, 1997; 30A:221 [7] Jin Z M, Hao Y C, Xu G. Acta Matall Sin, 2000; 36 : 391 (金珠梅,赫翼成,徐 广.金属学报, 2000;36:391) [8] Miao Y C, Di H S, Zhang X M, Bao P W, Wang G D, Liu X H. Res Iron Steel, 2000; (2): 32 (苗雨川,邸洪双,张晓明,鲍培玮,王国栋,刘相华.钢铁研 究,2000;(2):32) [9] Bouchuard D, Busque F. 82nd steelmaking conference:1999 Proceedings, 1999: 427 [10] Wen G H, Zhu M M, He J F, Li G, Han Z W, Ding P D. Acta Metal Sin, 2000; 36 : 1001 (文光华,祝明妹,何俊范,李 刚,韩志伟,丁培道.金属学 报,2000;36:1001) [11] Chen F, Duan Z L,Wang W A.Experiments of Material Mechanics.Wuhan:Huazhong University of Science and Technology Press, 1999: 345 (陈锋,段自力,王文安.材料力学实验.武汉:华中理工大 学出版社,1999:133) [12] Hu H, Zhao H M, Zhang J M, Wang X H, Wang W J. Iron Steel Vanadium Titanium, 2005; 26 (1): 10 (胡皓,赵和明,张炯明,王新华,王万军.钢铁钒钛.2005; 26(1):10) [13] Huang W X, Chen W M. Engineering Hydrodynamics. Beijing: Chemical Industry Press, 2001: 65 (黄卫星,陈文梅.工程流体力学.北京:化学工业出版社,2001: 65) [14] Kollberq S G, Hackl H R,Hamley P J. Iron Steel Eng, 1996; 73 (7): 24 |