| CBED Study of Local Strain Distribution in and Phases of a Crept Ni Base Superalloy |
| LÜ Zheng; F. Pyczak; H. Biermann; H. Mughrabi |
| Institut fu Werkstoffwissenschaften; Lehrstuhl I;Universitat Erlangen--Nurnberg; 91058 Erlangen; Germany |
|
Cite this article:
LÜ Zheng; F. Pyczak; H. Biermann; H. Mughrabi. CBED Study of Local Strain Distribution in and Phases of a Crept Ni Base Superalloy. Acta Metall Sin, 2006, 42(7): 694-698 .
|
|
|
Abstract The high lateral resolution CBED method was applied to measure the local elastic strain distributions in the two phases g and g¢ of the monocrystalline nickel-base superalloy CMSX-6 crept at 980℃. CBED measurements show that there is a difference of elastic strain in the vertical and horizontal g channels, which is thought to be the driving force for rafting. An inhomogeneous distribution of elastic strains is also observed in the g¢ phase.
|
|
Received: 15 November 2005
|
|
|
[1] Kuhn H A,Biermann H,Ungar T,Mughrabi H.Acta Metall Mater,1991; 39: 2783 [2] Biermann H,von Grossmann B,Ungar T,Mechsner S,Souvorov A,Drakopoulos M,Snigirev A,Mughrabi H. Acta Mater,2000;48: 2221 [3] Glatzel U, Muller A.Scr Metall Mater, 1994; 31: 285 [4] Volkl R,Glatzel U,Feller-Kniepmeier M.Acta Mater,1998; 46: 4395 [5] Keller R R,Maier H J,Renner H,Mughrabi H.Scr Metall Mater, 1992; 27: 1176 [6] von Grossmann B,Biermann H, Mughrabi H.Philos Mag,2000; 80A: 1743 [7] Von Grossmann B, Biermann H,Tetzlaff U,Pyczak F,Mughrabi H. Scr Mater, 2000; 43: 859 [8] Keller R R, Maier H J, Renner H, Mughrabi H. Scr Metall Mater, 1993; 28: 661 [9] Muller L, Link T, Feller-Kniepmeier M. Scr Metall Mater,1992; 26: 1297 [10] Zuo J M. Ultramicroscopy, 1992; 41: 211 [11] Krumer S,Mayer J.AIP Confer Proc,1999; 491: 289 [12] Stadelmann P.Ultramicroscopy,1987;21:131 [13] Carry C,Dermarkar S,Strudel J L,Wonsiewicz B G. Metell Trans, 1979; 10 A: 855 [14] Biermann H,Strehler M,Mughrabi H.Metell Mater Trans, 1996; 27A: 1003 [15] Kamaraj M, Mayer C,Kolbe M,Eggeller G. Scr Matter, 1998; 38: 589 [16] Mughrabi H, In: Arsenault R J, Cole D, Gross T, Kostorz G, Liaw P K,Parameswaran S P,Sizek H eds., The Johannes Weertman Symposium,Warrendale Pennsylvania: Minerals,Metals and Materials Society,1996: 267 [17] Buffiere J Y,Ignat M. Acta Matall Mater,1995; 43:1791 [18] Saito M,Aoyoma T,Hidaka K,Tamaki H,Ohashi T, Nakamura S,Suzuki T.Scr Mater,1996;34:1189 [19] Zhang Y,Wanderka N,Schumacher G,Schneider R,Neumann W.Acta Mater,2000;48:27871 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|