Abstract Mode II dynamic fracture toughnesses K IId for high strength
steels, 40Cr and 30CrMnSiNi2A, subjected to impact loading were measured
using an experiment-number combined method. The tests were performed
on shear specimens with Hopkinson pressure bar and the time of crack
initiation was determined by strain gauge. With 3-D transient finite
element analysis, the time evolution of dynamic stress intensity factor
under different loading rates was obtained and the dynamic fracture
toughness was determined by fracture initiation time. The results show
that within the loading rate range
(2×10 6 -7×10 6 MPa m 1/2/s),
almost all the specimens failed by adiabatic shear bands and the
K IId values of the two steels increase with
increasing loading rate. The K IId value of 30CrMnSiNi2A is
larger than that of 40Cr at the same loading rate. The effect of ligament
size on fracture toughness was also discussed.
|
Received: 29 September 2005
|
|
[1] Rokach I V. Fatigue Pract Eng Mater Struct, 1998; 21: 1007 [2] Li Y L. Rare Met Mater Eng, 1993; 22(5): 12 (李玉龙.稀有金属材料与工程, 1993;22(5):12) [3] Li Y L, Guo W G, Jia D X, Liu Y Y. Acta Mech Solid Sin, 1995; 8(Special Issue): 210 [4] Li Y L, Liu Y Y. J Comput Struct Mech Appl, 1995; 12(1): 110 (李玉龙,刘元镛.计算结构力学及应用, 1995;12(1):110) [5] Guo W G, Li Y L, Liu Y Y. Theor Appl Pract Mech, 1997; 26: 29 [6] Kalthoff J F, Winkler S. In: Chen C Y, Kunze H D, Meyer L W, eds., Proc Int Conf on Impact Loading & Dynamic Behavior of Materials, Bremen: Deutsche Gesellschaft fur Metallkunde, 1988: 185 [7] Kalthoff J F, Andreas B. Int J Fract, 2004; 30: 957 [8] Dong X L, Wang L L, Wang W, Yu J L. Explosion Shock Waves, 1999; 19: 222 (董新龙,王礼力,王 悟,虞吉林.爆炸与冲击, 1999;19: 222) [9] Dong X L, Wang L L, Yu J L. J Ningbo Univ (Nat Sci Eng Engl), 2003; 16: 429 [10] Ruiz C, Mines RAW. Int J Fract, 1985; 29: 101 [11] Rittel D, Levin R, Maigre H. Mech Res Commun, 1997; 24: 57 [12] Klepaczko J R. J Mech Phys Solids, 1998; 46: 2139 [13] Mercier S, Molinari A. J Mech Phys Solids, 1998; 46: 1463 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|