| Near Threshold Fatigue Crack Propagation Under Combined Torsion And Tension In Stainless Steel |
| HuiChen Yu |
| 北京航空材料研究院 |
|
Cite this article:
HuiChen Yu. Near Threshold Fatigue Crack Propagation Under Combined Torsion And Tension In Stainless Steel. Acta Metall Sin, 2006, 42(2): 186-190 .
|
|
|
Abstract Near-threshold fatigue crack propagation tests were conducted under combined torsion and tension on a circumferentially pre-cracked round bar of an austenite steel. The propagation behavior was studied extensively under various combinations of cyclic loads. The threshold condition of fatigue crack extension was expressed by a quarter-elliptic function in terms of the stress intensity factor ranges for mode I and III. The equation can be derived on the basis of the crack-tip displacement criterion. The threshold condition for fracture is also expressed by another quarter-elliptic function.
|
|
Received: 26 May 2005
|
|
|
[1] Pook L P. Int J Fatigue, 1985; 7: 21 [2] Yates J R, Miller K J. Fatigue Fract Eng Mater Struct, 1989; 12: 259 [3] Yoshioka S, Watanabe K, Kitagawa H, Inoue A, Kumasawa M. Trans Jpn Soc Mech Eng, 1984; 50: 1267 [4] Tschegg E K. Mater Sci Eng, 1982; 54: 127 [5] Tschegg E K. J Mater Sci, 1983; 18: 1604 [6] Yu H C, Tanaka K, Akiniwa Y. Fatigue Fract Eng Mater Struct, 1998; 21: 1067 [7] Yu H C, Zhang Y J, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 721(于慧臣,张岩基,谢世殊,田中启介.金属学报,2005;41:7211 [8] Yu H C, Tanaka K, Akiniwa Y. In: Senoo M, Xu B Y, Tokuda M, Bundara B, eds., Proc 3rd Int Symp on Microstructures and Mechanical Properties of New Engineering Materials (IMMM'97), Tsu, Japan: Mie University Press, 1997: 309 [9] Ritchie R O, McClintock F A, Hayeb-Hashemi H, Ritter M A. Metall Trans, 1982; 13A: 101 [10] Yu H C, Sun Y G, Xie S S, Tanaka K. Acta Metall Sin, 2005; 41: 73(于慧臣,孙燕国,谢世殊,田中启介.金属学报,2005;41:73) [11] Tada H, Paris P C, Irwin G R. The Stress Intensity Factor Handbook. 2nd ed, Hellertown, Philadelphia: Del Research Corporation, 1985; 27: 3 [12] Rice J R. ASTM STP 415, 1967: 247 [13] Brown M W, Hay E, Miller K J. Fatigue Fract Eng Mater Struct, 1985; 8: 243 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|