| Nano-crystallization in Amorphous Material under Compression Deformation: A Molecular Dynamics Study |
| Wang Yu;; |
| 中国科学技术大学力学和机械工程系;中科院材料行为和研究重点实验室 |
|
Cite this article:
Wang Yu. Nano-crystallization in Amorphous Material under Compression Deformation: A Molecular Dynamics Study. Acta Metall Sin, 2006, 42(10): 1071-1074 .
|
|
|
Abstract The nano-crystallization behavior of amorphous pure Ni under compression deformation has been investigated by using a molecular dynamics simulation. The effect of adiabatic procedure on the nano-crystallization was studied. The nucleation and growth of nano crystal was observed by through the evolution of micro structure. It was shown that the transition from the metastable structure to crystal structure was driven by the compression deformation. The shorted ordered clusters combined and grew into the nano-crystal with the strain increasing.
|
|
Received: 23 January 2006
|
|
|
[1]Inoue A.Acta Mater,2000;48:279 [2]Johnson W L.MRS Bull,1999;24:42 [3]Loffler J F.Intermetallics,2003;11:529 [4]Zhang Z F,Eckert J,Schultz L.Acta Mater,2003;51:1167 [5]Chen H,He Y,Shiflet G J,Pooh S J.Nature,1994;367:541 [6]Jiang W H,Atzmon M.Acta Mater,2003;51:4095 [7]Kim J J,Choi Y,Suresh S,Argon A S.Science,2002;295:654 [8]Hebert R J,Perepezko J H.Mater Sci Eng,2004;A375-377:728 [9]Baskes M I.Phys Rev,1992;46B:2727 [10]Daw M S,Baskes M I.Phys Rev Lett,1983;50:1285 [11]Daw M S,Baskes M I.Phys Rev,1984;29B:6443 [12]Qi L,Zhang H F,Hu Z Q.Acta Metall Sin,2004;40:736(戚力,张海峰,胡壮麒.金属学报,2004;40:736) [13]Honeycutt J D,Andersen H C.J Phys Chem,1987;91:4950 [14]Lu K,Wang J T.Acta Metall Sin,1991;27:38(卢柯,王景唐.金属学报,1991;27:38) [15]Qi Y,Cagin T,Kimura Y,Goddard W AⅢ.Phys Rev,1999;59B:3527 [16]Schuh C A,Lund A C.Nat Mater,2003;2:449 [17]Shi Y F,Falk M L.Appl Phys Lett,2005;86:011914 [18]Lu K,Wang J T,Dong L.Acta Metall Sin,1991;27:31(卢柯,王景唐,董林.金属学报,1991;27:31)7 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|