| Effect of La on the Mechanical Property and Corrosion Resistance of AZ91D |
| FAN Yu; WU Guohua; GAO Hongtao; LI Guanqun; ZHAI Chunquan |
| State Key Laboratory of Metal Matrix Composite; Shanghai Jiaotong University; Shanghai 200030 |
|
Cite this article:
FAN Yu; WU Guohua; GAO Hongtao; LI Guanqun; ZHAI Chunquan. Effect of La on the Mechanical Property and Corrosion Resistance of AZ91D. Acta Metall Sin, 2006, 42(1): 35-42 .
[1]Mathieu S,Rapin C,Steinmerz J,Steinmetz P.Corros Sci,2003;45:2741 [2]Ambat R,Aung N N,Zhou W.Corvos Sci,2000;42:1433 [3]Aung N N,Zhou W J.Appl Electrochem,2002;32:1397 [4]Jinko Y,Yim C D,Lim J D.Mater Sci Forum,2003;419-422:851 [5]Song G L,St John D J.Light Met,2002;2:1 [6]Nakatsugawa I,Kamado S,Kojima Y,Ninomiya R,Kubota K.Corros Rev,1998;16:558 [7]Lunder O,Lein J E,Aune T Kr,Nisancioglu K.Corrosion,1989;45:741 [8]Song G L,Atrens A,Dargush M.Corros Sci,1999;41:249 [9]Song G L,Bowles A L,Stjohn D H.Mater Sci Eng,2004;A366:74 [10]Mathieu S,Rapin C,Steinmerz J,Steinmetz P.Corros Sci,2002;44:2737 [11]Makar G L,Kruger J.Int Mater Rev,1993;38:138 [12]Song G,Atrens A,Wu X,Zhang B.Corros Sci,1998;40:1769 [13]Song G,Atrens A,St John D,Wu X.J Naim.Corros Sci,1997;39:1981 [14]Makar G L,Kruger J,Joshi A.Advances in Magnesium Alloys and Composites.TMS,1988:105 [15]Bonora P L,Andrei M,Eliezer A,Gutman E M.Corros Sci,2002;44:729 [16]Udhayan R,Devendra P B.J Power Sources,1996;63:103a |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|