| In Situ Raman Spectroscopy Observation for Domain Switching of Ferroelectric Ceramics |
| ZHANG Sa; CHENG Xuan; ZHANG Ying |
| Department of Chemistry; Xiamen University; Xiamen 361005 |
|
Cite this article:
ZHANG Sa; CHENG Xuan; ZHANG Ying. In Situ Raman Spectroscopy Observation for Domain Switching of Ferroelectric Ceramics. Acta Metall Sin, 2005, 41(6): 663-668 .
|
|
|
Abstract In order to develop a nondestructive technique
observing domain switchings in microscopic scale, an in situ
method was proposed based upon the principal of Raman
spectroscopy. Two types of experiments were carried out to verify the
proposed method. One is to measure
the Raman spectra for a fixed grain in the PLZT ferroelectric
sample before and after 90
rotation. The other is to observe variations of Raman spectra for a fixed
grain under a DC field. The results revealed that by a 90 rotation
the Raman
spectra for grains in an in-plane polarized sample vary and the Raman spectra
for grains in both un-poled and out-plane polarized samples remain unchanged.
The results also indicated that the in situ Raman spectrum varies as the
magnitude of the applied DC field increases. These results showed
that the domain switching will leads to variations of Raman spectrum.
|
|
Received: 09 October 2004
|
|
|
[1]Zhang Y,Chen Z W,Cheng X,Zhang S.Acta Metall Sin,2004;40:1299 (张颖,陈志武,程璇,张飒.金属学报,2004;40:1299) [2]Chen Z W.Doctor's Dissertation,Xiamen University,2003 (陈志武.厦门大学博士学位论文,2003) [3]Tan X L,Xu Z K,Shang J K.Mater Sci Eng,2001;A314:157 [4]Zhong W L.Physics of Ferroelectrics.Beijing:Science Press,1996:155 (钟维烈.铁电物理学.北京:科学出版社,1996:155) [5]Zhang G Y,Lan G X,Wang Y F.Spectroscopy of Lattice Vibrations.Beijing:Higher Education Press,2001:195 (张光演,蓝国祥,王玉芳.晶格振动光谱学.北京:高等教育出版社,2001:195) [6]Fang R C.Spectroscopy of Solids.Hefei:University of Science and Technology of China Press,2001:282 (方容川.固体光谱学.合肥:中国科学技术大学出版社,2001:282) [7]Wright G H.Light Scattering of Solids.New York:Springer,1962 [8]Burns G,Scott B A.Phys Rev Lett,1970;23:167 [9]Burns G,Scott B A.Phys Rev Lett,1970;23:1191 [10]Burns G,Scott B A.Phys Rev,1973;7B:3088 [11]Fontana M D,Idrissi H,Kugel G E,Wojcik K.J Phys Condens Matter,1991;3:8695 [12]Pasto A E,Condrate R E.J Am Ceram Soc,1973;56:436 [13]Bismayer U.Phase Transit,1990;27:211 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|