| Oxidation of Fe-xCr-10Al (x=0, 5, 10) Alloys at 900 ℃: A Novel Example of the Third Element Effect |
| ZHANG Zhigang; P.Y. Hou; NIU Yan |
| State Key Laboratory for Corrosion and Protection; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110016 |
|
Cite this article:
ZHANG Zhigang; P.Y. Hou; NIU Yan. Oxidation of Fe-xCr-10Al (x=0, 5, 10) Alloys at 900 ℃: A Novel Example of the Third Element Effect. Acta Metall Sin, 2005, 41(6): 649-654 .
|
|
|
Abstract The critical Al content for the selective formation of
alumina scales on Fe-Al alloys has been analyzed by investigating
the oxidation behavior of binary Fe-10Al and ternary
Fe-5Cr-10Al and Fe-10Cr-10Al alloys (atomic fraction, %).
A possible interpretation of the effect of
the third-element Cr in Fe-xCr-10Al on
promoting Al2O3 scale formation not involving a transition
from the internal to external oxidation of Al is briefly presented.
|
|
Received: 25 November 2004
|
|
|
[1]Hindam H,Whittle D P.Oxid Met,1982;18:245 [2]Tomaszewicz P,Wallwork G R.Oxid Met,1983;20:75 [3]Boggs W E.J Electrochem Soc,1971;118:906 [4]Hagel W C.Corrosion,1965;21:316 [5]Ahmed H A,Smeltzer W W.J Electrochem Soc,1986;133:212 [6]Saegusa F,Lee L.Corrosion,1966;22:168 [7]Ahmed H A,Underhill R P,Smeltzer W W,Brett M E, Graham M J.Oxid Met,1987;28:347 [8]Tomaszewicz P,Wallwork G R.Oxid Met,1983;19:165 [9]Hou P Y,Stringer J.Oxid Met,1992;38:323 [10]Miner R G,Nagarajan V.Oxid Met,1981;16:313 [11]Stott F H,Wood G C,Hobby M G.Oxid Met,1971;3:103 [12]Golightly F A,Wood G C,Stott F H.Oxid Met,1980;14:217 [13]Lambertin M,Stoklosa A,Smeltzer W W.Oxid Met,1981; 15:355 [14]Sadique S E,Mollah A H,Islam M S,AH M M,Megat M H H,Basri S.Oxid Met,2000;54:385 [15]Stott F H,Wood G C,Stringer J.Oxid Met,1995;44:113 [16]Wagner C.Corros Sci,1965;5:751 [17]Zhang Z G,Gesmundo F,Hou P Y,Niu Y.Corros Sci,2005,in press [18]Wagner C.J Electrochem Soc,1952;99:369 [19]Gesmundo F,Niu Y.Oxid Met,1998;50:1 [20]Crank J.The Mathematics of Diffusion.New York:Oxford University Press,1994 [21]Takada J,Yamamoto S,Kikuchi S,Adachi M.Oxid Met,1986;25:93 [22]Carslaw H S,Jaeger J C.Conduction of Heat in Solids,New York:Oxford University Press,1993 [23]Graham M J,Eldrige J I,Mitchell D F,Hussey R J.Mater Sci Forum,1989;43:207 [24]Niu Y,Gesmundo F.Oxid Met,2001;56:517 [25]Levin E M,Robbins C R,McMurdie H F.Phase Diagrams for Ceramists.Columbus:The American Ceramic Society,1969 [26]Niu Y,Gesmundo F.Oxid Met,in press |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|