| Effect of P2O5 on Interfacial Oxygen Transfer Reaction and Its Mechanism |
| HU Xiaojun |
| Department of Physical Chemistry; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
HU Xiaojun. Effect of P2O5 on Interfacial Oxygen Transfer Reaction and Its Mechanism. Acta Metall Sin, 2005, 41(6): 655-658 .
|
|
|
Abstract The rate constant of oxygen transfer reaction between the molten iron
oxide and CO2 gas on the surface of liquid slag was measured by
the isotope exchange method. Also, according to the electrochemical
mechanism in the reaction process, the effect of P2$O5 additive
was discussed and a new model was established. From this model, due to
participating the electron competition while volatilizing from slag,
P2$O5 decreases the oxygen transfer rate. The results of
analyzing and fitting to the experimental data have indicated that
this new model is available to explain the effect of P2O5,
and supported the view which there exits an electrochemical mechanism
in this process.
|
|
Received: 24 September 2004
|
|
|
[1]Nagasaka T,Tguchi Y.Ban-ya S.Tetsu Hagane,1989;75:74 (长坂徹也,井口(?)孝,乃谷 志郎 铁 钢,1989;75:74) [2]Sun S,Belton G R.Metall Mater Trans,1998;29B:137 [3]Matsuzaki K,Maki T,Hamano T,Ito K.Metall Mater Trans,1999;30B:827 [4]Cramb A W,Graham W R,Belton G R.Metall Trans, 1978;9B:623 [5]Matsuura H,Ishida I,Tsukihashi F.ISIJ Int,2004;44:1494 [6]Belton G R.Metall Trans,1976;7B:35 [7]Woolley D E,Pal U B.Metall Mater Trans,1999;30B:877 [8]Woolley D E,Pal U B.Ironmaking Steelmaking,2002;29:125 [9]Kambayashi S,Awaka A.Kato E.Tetsu Hagane,1985;71:1911 (神林茂,阿波加博俊,加藤栄 铁 钢,1989;71:1911) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|