Formation Mechanism of Band Structure and Phase Selection During Directional Solidification of Peritectic Alloys I.Formation Mechanism of Band Structure |
LI Xinzhong; GUO Jingjie; SU Yanqing; WU Shiping; FU Hengzhi |
School of Materials Science and Engineering; Harbin Institute of Technology; Harbin 150001 |
|
Cite this article:
LI Xinzhong; GUO Jingjie; SU Yanqing; WU Shiping; FU Hengzhi. Formation Mechanism of Band Structure and Phase Selection During Directional Solidification of Peritectic Alloys I.Formation Mechanism of Band Structure. Acta Metall Sin, 2005, 41(6): 593-598 .
|
Abstract Solute compositional distributions at and ahead of the solid--liquid
interfaces are analyzed during the plane--front growth for both the
primary and peritectic phases as single phase and nucleation phase
for peritectic alloys directionally solidified at low growth rates
from initial transient to steady state. Taking the nucleation and
compositional undercooling criterion and assuming that the maximum
interface growth temperature of phase growth is more stability during
the directional solidification, the nucleation transitions during the
transient period are investigated and compositional range of band
structure formation is determined. Considering the history--dependant
growths of a phase, the band structure can be differentiated as cycling
band and single band structure, which can explain the experimental
phenomena appropriately. The calculated results for Ti-Al alloy are
identical with the theoretical analyses.
|
Received: 15 September 2004
|
|
[1]Boettinger W J.Metall Trans,1974;5:2023 [2]Brody H D,David S A.In:Solidification and Casting of Metals,London:The Metals Society,1979:144 [3]Titchener A P,Sppittle J A.Acta Metall,1975;23:497 [4]Ostrowski A,Langer E W.In:Solidification and Casting of Metals,London:The Metals Society,1979:139 [5]Trivedi R.Metall Trans,1995;26A:1583 [6]Zeisler-Mashl K L,Lograsso T A.Metall Mater Trans,1997;28A:1543 [7]Kurz W,Trivedi R.Metall Mater Trans,1996;27A:625 [8]Tokieda K,Yasuda H,Obanaka I.Mater Sci Eng,1999;A262:241 [9]Li S M,Liu L,Li X L,Fu H Z.Acta Metall Sin,2004;40:20 (李双明,刘林,李晓历,傅恒志.金属学报,2004;40:20) [10]Umeda T,Okane T.Sci Technol Adv Mater,2001;2:239 [11]Karma A,Rappel W-J,Fuh B C,Trivedi R.Metall Mater Trans,1998;29A:1457 [12]Hunziker O,Vandyoussefi M,Kurz W.Acta Mater,1998;46:6325 [13]Tiller W A.The Science of Crystallization:Macroscopic Phenomena and Defect Generation.Cambridge:Cambridge University Press,1991:143 [14]Zhang F,Chen S L,Chang Y A.In:Kim Y W,Wagner R,Yamaguchi M,eds.,Gamma Titanium Aluminides.War-rendale,PA:The Minerals,Metals & Materials Society,1995:131 |