| Low Cycle Fatigue Behavior Of Cast Nickel Base Superalloy K52 |
| YAO Jun; GUO Jianting; YUAN Chao; LI Zhijun |
| Institute of Metal Research; The Chinese Academy of Sciences; Shenyang110016 |
|
Cite this article:
YAO Jun; GUO Jianting; YUAN Chao; LI Zhijun. Low Cycle Fatigue Behavior Of Cast Nickel Base Superalloy K52. Acta Metall Sin, 2005, 41(4): 357-362 .
|
|
|
Abstract Low cycle fatigue (LCF) behaviors of cast nickel-base superalloy K52
at different temperatures were investigated, and the fatigue parameters
were given by analyzing its cyclic stress-strain curves and
strain-life curves. Cyclic stress response curves show that the alloy
exhibited cyclic hardening and softening behaviors at room temperature
and 900℃, respectively. OM and SEM observations indicated that LCF cracks
initiated predominantly on the surface of specimen or at the near-surface
defects. Once initiated, cracks would propagate perpendicularly to the
loading direction and the specimens exhibited transgranular fracture.
|
|
Received: 09 October 2004
|
|
|
[1]Miller H E, Chambers W L. In: Sims C T, Ctoloff N S, Hagel W G, eds., Superalloy Ⅱ, New York: John-Wiley & Sons, 1987: 18 [2]Reuchet J, Remy L. Mater Sci Eng, 1983; 58: 19 [3]Bhanu Sankara Rao K, Schiffers H, Schuster H, Nickel H. Metall Trans, 1988; A19: 359 [4]Valsan M, Shastry D H, Bhanu Sankara Rao K, Mannan S L. Metall Trans, 1994; 25A: 159 [5]Li S X, Smith D J. Fatigue Fract Eng Mater Struct, 1995; 18: 631 [6]Lerch B A, Gerold V. Metall Trans, 1987; ISA: 2135 [7]Valsan M, Paramewaran P, Bhanu Sankara Rao K, Vijay alakshmi M, Mannan S L, Sastry D H. Metall Trans, 1992; 23A(6): 1751 [8]Gayda J, Miner R V. Int J Fatigue, 1983; 5: 135 [9]Burke M A, Beck C G. Metall Trans, 1984; 15A: 661 [10]Standard E606. In: Annual Book of ASTM Standards, Philadelphia, PA: ASTM, 1996; 03.01 [11]Chen L J, Wang Z G, Yao G, Tian J F. Acta Metall Sin, 1999; 35: 1144 (陈立佳,王中光,姚戈,田继丰.金属学报,1999;35:1144) [12]Yang F M, Sun X F, Guan H R, Hu Z Q. Acta Metall Sin, 2002; 38: 1047 (杨富民,孙晓峰,管恒荣,胡壮麒.金属学报,2002;38:1047) [13]Guo J T, Ranucci D, Picco E. Mater Sci Eng, 1983; 58: 127 [14]Guo J T, Ranucci D, Picco E, Strocchi P M. Int J Fatigue, 1984; 6: 95 [15]Hwang S K, Lee H N, Yoon B H. Metall Trans, 1989; 20A: 2793 [16]Antolovich S D, Liu S, Baur R. Metall Trans, 1981; 12A: 473 [17]Calabrese C, Larid C. Mater Sci Eng, 1974; 13: 141 [18]Remy L, Reuchet J. Mater Sci Eng, 1983; 58: 19 [19]Fournier D, Pineau A. Metall Trans, 1977; 8A: 1095P |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|