CRYSTAL STRUCTURE AND MICROSTRUCTURE OF RAPIDLY SOLIDIFIED La(Ni, Sn)(5+x)(x=0.1---0.4) HYDROGEN STORAGE ALLOYS
Cite this article: 

. CRYSTAL STRUCTURE AND MICROSTRUCTURE OF RAPIDLY SOLIDIFIED La(Ni, Sn)(5+x)(x=0.1---0.4) HYDROGEN STORAGE ALLOYS. Acta Metall Sin, 2004, 40(8): 805-809 .

Download:  PDF(259KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  01 January 1900     
ZTFLH:  TG139.7  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I8/805

[1] Notten P H L, Einerhand R E F, Daams J L C. J AlloyCompds, 1994; 210: 221
[2] Vogt T, Reilly J J, Johnson J R, Adzic G A, MeBreen J.Electrochem Solid-State Lett 1999; 2(3) : .111
[3] Higashiyama N, Matsuura Y, NaKamura H, Kimoto M,Nogami M, Yonezu I, Nishio K. J Alloys Compds, 1997;253-254: 648
[4] Li C, Wang X L, Wang C Y. J Alloys Compds, 1999; 293295: 742
[5] Lei Y Q, Zhang S K, Lu G L, Wang Q D. J Alloys Compds,2002; 330-332: 861
[6] Zhang S K, Shu K Y, Lei Y Q, Lu G L, Wang Q D. InterJ Hydro Ener, 2003; 28: 977
[7] Wiles D B, Young R A. J Appl Cryst, 1981; 149: 14
[8] Keijser Th H de, Langford J I, Mittemeijer E J, Vogels AB P. J Appl Cryst, 1982; 15: 308
[9] Keijser Th H de; Mittemeijer E J, Rozendaal H C F. JAppl Cryst, 1983; 16: 309
[10] Lartigue C, Le Bail A, Percheron-GueganA. J LessCommon Met, 1987; 129: 65
[11] Popa N C. J Appl Cryst, 1992; 25: 611
[12] Popa N C. J Appl Cryst, 1998; 31: 176
[13] Ferrari M, Lutterotti L. J Appl Phys, 1994; 76(11) : 7246
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!