Acta Metall Sin  2004, Vol. 40 Issue (8): 799-804     DOI:
Research Articles Current Issue | Archive | Adv Search |
EFFECT OF EXTERNAL STRESS ON THE GROWTH OF PRECIPITATES IN Al--Cu AND Al--Cu--Mg--Ag ALLOYS
Cite this article: 

. EFFECT OF EXTERNAL STRESS ON THE GROWTH OF PRECIPITATES IN Al--Cu AND Al--Cu--Mg--Ag ALLOYS. Acta Metall Sin, 2004, 40(8): 799-804 .

Download:  PDF(295KB) 
Export:  BibTeX | EndNote (RIS)      
Key words:       
Received:  01 January 1900     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2004/V40/I8/799

[1] Bogers A J. Acta Metali, 1962; 10: 260
[2] Hosford W F, Agrawal S P. Metali Trans, 1975; 6A: 4879
[3] Eto T, Sato A, Mori T. Acta Metali, 1978; 26: 499
[4] Tanaka Y, Sato A, Mori T. Acta Metali, 1978; 26: 529
[5] Skrotzki B, Shiflet G J, Starke E A Jr. Metall MaterTrans, 1996; 27A: 3431
[6] Zhu A W, Starke E A Jr. Acta Mater, 2001; 49: 2285
[7] Miyazaki T, Nakamura K, Mori H. J Mater Sci, 1979; 14:1827
[8] Nishizawa H, Sukedai E, Liu W, Hashimoto H. MaterTrans JIM, 1998; 39: 609
[9] Mukhopadhyay A K, Murken J, Skrotzki B, Eggeler G.Mater Sci Forum, 2000; 331-337: 1555
[10] Li D Y, Chen L Q. Acta Mater, 1998; 46: 2573
[11] Rossiter P L. The Electrical Resistivity of Metals and Alloys, London: Cambridge University Press, 1987: 107
[12] Hull S, Messoloras S, Stewart R J. Phil Mag A, 1988; 57:261
[13] Suh I S, Park J K. cer Metall Mater, 1995; 33: 205
[14] Reich L, Murayama M, Hono K. Acta Mater, 1998; 46: 6053
[15] Huchinson C R, Fan X, Pennycook S J, Shiflet G J. ActaMater, 2001; 49: 2827
[16] Ringer S P, Yeung W, Muddle B C, Polmear I J. ActaMetali Mater, 1994; 42: 1715
[17] Howe J M. Philos Mag Lett, 1994; 70: 111
[18] Fonda R W, Cassada W A, Shiflet G J. Acta Metali Mater,1992; 40: 2539
[19] Eshelby J D. Proc R Soc A, 1957; 241, 376
[20] Eshelby J D. Proc R Soc A, 1959; 252, 561
[21] Eshelby J D. Prog Solid Mech, 1961; 2, 87
[22] Mura T. Micromechanics of Defects in Solids, 2nd edition,Dordrech: Martinus Nijhoff, 1987: 177
[23] Fukikawa S, Hirano K. Defect and Diffusion Forum,Brandrain: Trans Tech Publications Ltd, 1989; 66-69: 447
[24] Dahmer U, Westmacott K H. Phys Status Solidi (a), 1983;80: 249
[25] Stobbs W M, Purdy G R. Acta Metall, 1978; 26: 1069
[1] WANG Luning, LIU Lijun, YAN Yu, YANG Kun, LU Lili. Influences of Protein Adsorption on the in vitro Corrosion of Biomedical Metals[J]. 金属学报, 2021, 57(1): 1-15.
[2] TUNG Feng'en;WANG Yuming Institute of Materials Science; Jilin University; Changchun. X-RAY ANALYSIS OF WORK-HARDENING PROCESS FOR POLYCRYSTALLINE а-BRASS DURING UNIAXIAL TENSILE TEST[J]. 金属学报, 1989, 25(2): 82-84.
[3] WANG Jinliang, WANG Chenchong, HUANG Minghao, HU Jun, XU Wei. The Effects and Mechanisms of Pre-Deformation with Low Strain on Temperature-Induced Martensitic Transformation[J]. 金属学报, 2021, 57(5): 575-585.
[4] DU Hegui;LIU Xin Northeast University of Technology; Shenyang. KINETICS OF CARBON COMBUSTION IN PLASMA AIR[J]. 金属学报, 1989, 25(2): 85-88.
[5] . [J]. 金属学报, 2001, 37(1): 42-46 .
[6] . [J]. 金属学报, 1999, 35(3): 320-324 .
[7] . [J]. 金属学报, 2000, 36(1): 72-76 .
[8] . [J]. 金属学报, 1999, 35(3): 330-333 .
[9] . [J]. 金属学报, 1999, 35(3): 334-336 .
[10] . [J]. 金属学报, 2000, 36(6): 647-650 .
[11] . [J]. 金属学报, 2000, 36(6): 655-658 .
[12] No Author. ACTA METALLURGLCA SLNLCA Volume 28 Series A 1992 SUBJECT INDEX[J]. 金属学报, 1992, 28(12): 63-90.
[13] . [J]. 金属学报, 2000, 36(7): 780-784 .
[14] No Author. ACTA METALLURGICA SINICA(JINSHU XUEBAO) Volume 28 1992 AUTHOR INDEX[J]. 金属学报, 1992, 28(12): 71-94.
[15] Хань Яо-вэнь Инсмцмум мемаддов АН КНР;Г.н.Ойкс Московскц цнсмцмум смадц. НЗУЧЕНИЕ ПРОЦЕССОВ ДЕСУЛЬФУРАЦИИ ХНДКОΓО МЕТАЛЛА В ВАКУУМЕ[J]. 金属学报, 1963, 6(2): 98-110.
No Suggested Reading articles found!