| Thermodynamic Modeling for Controls of Deoxidation and Oxide Inclusions in Molten Steel |
| ZHANG Xiaobing |
| Technology Center; Shanghai No.1 Iron & Steel Co.; Baosteel Group; Shanghai 200431 |
|
Cite this article:
ZHANG Xiaobing. Thermodynamic Modeling for Controls of Deoxidation and Oxide Inclusions in Molten Steel. Acta Metall Sin, 2004, 40(5): 509-514 .
|
|
|
Abstract Component activities in CaO-MgO-Al2O3-SiO2
and CaO-MnO-Al2O3-SiO2 systems were calculated
by a sub-regular solution model of a multi-component system.
A thermodynamic modeling for controls of deoxidation and oxide
inclusion in molten steel was developed based on these calculations,
which was used for thermodynamic calculations for deoxidation,
slag-melt equilibration and oxide-melt equilibration
in order to control the deoxidation and compositions of
oxide inclusion of steel. The results of model
applications are validated with the industrial
database such as the silicon deoxidation through
slag-melt equilibration in LF, the calcium
treatment of Al-Si killed steel and the composition of
oxide inclusion formed during solidification in caster. The
presented modeling can be used in deoxidation
control and oxide inclusion control in steel.
|
|
Received: 26 May 2003
|
|
|
[1] The Japan Society for the Promotion of Science. Steelmaking Data Sourcebook, The 19th Committee on Steelmaking, New York: Gordon and Breach Science Publishers, 1988:280 [2] Ban-Ya S, Hiso M. Tetsu Hangané, 1988: 74:1701(万谷志郎,日野 光兀.铁钢,1988;74:1701) [3] Pelton A D, Blander M. In: Fine H A, Gashell D R, eds., 2nd Int Symp on Metallurgical Slag and Fluxed, New York: Metal Society AIME, 1984:281 [4] Hillert M, Jansson B, Sundman B. Metall Trans, 1990; 21B: 405 [5] Kapoor M K, Frohberg M G. In: Iron and Steel Institute, UK, ed., Symposium on Chemical Metallurgy of Iron and Steel. Sheffield, London, 1971:17 [6] Gaye H, Welfringer J. In: Fine H A, Gashell D R eds., 2nd Int Symp on Metallurgical Slag and Fluxed, New York: Metal Society AIME, 1984:357 [7] Pelton A D, Flengas S M. Can J Chem, 1969; 47:2283 [8] Zhang X B, Jiang G C, Xu K O. CALPHAD, 1997; 21: 311 [9] Gatellier C, Olette M. Rev Metall, 1979; 76:378 [10] Nadif M, Gatellier C. Rev Metall, 1986; 83:377 [11] Ban-Ya S, Hino M. Chemical Properties of Molten Slags, The Iron and Steel Institute of Japan, Tokyo, 1991:1 [12] Zhang X B, Jiang G C, Xu K D. Acta Metall Sin, 1997; 33:1085(张晓兵,蒋国昌,徐匡迪.金属学报,1997;33:1085) [13] Zhang X B, Jiang G C, Xu K D. In: Iron and Steel Society, USA, ed., The 5th Int Conf on Molten Slags, Fluxes and Salts 1997, Sydney, Australia, 1997:259 [14] Zhang X B, Jiang G C, Tang K, Ding W, Xu K D. CALPHAD, 1997; 21; 301 [15] Abraham K P, Davies M W, Richardson F D. J Iron Steel Inst, 1960; 196:82 [16] Sharma R A, Richardson F D. Trans AIME, 1965; 233: 586 [17] Risbud S H, Pask J A. J Am Ceram Soc, 1977; 60:418 [18] Rein R H, Chipman J. Trans AIME, 1965; 233:415 [19] Sharma R A, Richardson F D. J Iron Steel Inst, 1961; 198: 386 [20] Mehta S R, Richardson F D. J Iron Steel Inst, 1965; 203: 524 [21] Mogutnov B M, Zaitsev A I, Livina A D. In: Iron and Steel Society, USA, ed., 2nd Int Congress on the Science and Technology of Iron Making and 57th, Ironmaking Conference. Toronto, Canada, 22-25 March, 1998:1477 [22] Eriksson G, Pelton A D. Metall Trans, 1993; 24B: 807 |