| Numerical Simulation of Mold Filling and Solidification of TiAl Base Alloy Exhaust Valve in Vertical Centrifugal Casting Process |
| WU Shiping; GUO Jingjie; JIA Jun |
| School of Materials Science and Engineering; Harbin Institute of Technology |
|
Cite this article:
WU Shiping; GUO Jingjie; JIA Jun. Numerical Simulation of Mold Filling and Solidification of TiAl Base Alloy Exhaust Valve in Vertical Centrifugal Casting Process. Acta Metall Sin, 2004, 40(3): 326-330 .
|
|
|
Abstract Based on N--S function, continuity function, function of Fourier heat conduction and experiments, a mathematical model of mold filling and solidification in vertical centrifugal casting is presented by taking centrifugal force, gravity and Coriolis force into consideration. This model is further applied to numerical simulation of temperature field, flow field and pressure field of vertical centrifugal casting process of exhaust valve made of TiAl base alloy. The result of numerical simulation shows that the mold filling of vertical centrifugal casting consists of forward--direction filling and back--direction filling. Gas--holes defect easily appears at the entrance of valve. The two orders also exist in solidification proces and are major reason for formation of off—axis shrinkage nearby the side of filling first.
|
|
Received: 06 December 2002
|
|
|
[1] Sheng W B, Ding H S, Guo J J, Su Y Q, Jia J. Foundry, 2000: 49(3) :125(盛文斌,丁宏升,郭景杰,苏彦庆,贾均.铸造,2000;49(3) :125) [2] Sheng W B, Guo J J, Su Y Q, Chen H S, Jia J. Mater Sci Technol, 2001; 17(5) :569 [3] Murta k, Takada M, Nakata T, Nunomura S. Imono, 1992; 64(8) :537 [4] Yang G Z, Wei B K, Xu Z L, Lin H T, Yah Y W. Spec Cast Nonferrous Alloys, 1997; 2:11(扬光照,魏伯康,徐自立,林汉同,严有为.特种铸造及合金,1997;2:11) [5] Xu Z L, Yang G Z, Wei B K, Lin H T. Hot Work Technology, 1994; 6:5(徐自立,扬光照,魏伯康,林汉同.热加工工艺,1994;6:5) [6] Zhang B S, Chen H S, Lin B N, An G Y. Foundry, 1994; 1:1(张宝生,陈洪升,林柏年,安阁英.铸造,1994;1:1) [7] Wang Q D, Ding W J,Jin J Z, Chen Q Y,Yin Y S. Foundry, 1998; 10:16(王渠东,丁文江,金俊泽,陈秋勇,尹衍升.铸造,1998;10:16) [8] Zhang B S, Chen H S, An G Y, Lin B N. Foundry, 1995; 3:6(张保生,陈洪升,安阁英,林柏年.铸造,1995;3:6) [9] Jong S H, Hwang W S. AFS Trans, 1992; 100:489 [10] Xue X, Hansen S F, Hansen P N. AFS Trans, 1993; 101:549 [11] Jong S H, Hwang W S. AFS Trans, 1991; 99:117 [12] Song G M, Zhou Y, Sun Y, Lei T C. Ceram Int, 1998; 24(6) : 455 [13] Larsen D, Colvin G. J Miner Met Mater Soc, 1999; 6:26 [14] Wu S P, Guo J J, Su Y Q, Jia J. Foundry, 2001; 5:25(吴士平,郭景杰,苏彦庆,贾均.铸造,2001;5:25) |