| A New Nd--Based Bulk Metallic Glass |
| REN Yinglei; ZUO Jinghui;QIU Keqiang; ZHANG Haifeng; HU Zhuangqi |
| Faculty of Materials Science and Engineering; Shenyang University of Technology |
|
Cite this article:
REN Yinglei; ZUO Jinghui; QIU Keqiang; ZHANG Haifeng; HU Zhuangqi. A New Nd--Based Bulk Metallic Glass. Acta Metall Sin, 2004, 40(3): 301-304 .
|
|
|
Abstract A new Nd61Fe30Zn9 bulk metallic glass with a diameter of 2.5 mm was obtained using copper mold casting. No glass transition temperature or supercooled liquid region was observed by using conventional DSC--7 facility. The crystallization temperature for the bulk sample is 730 K, which is about 70 K lower than that of Nd60Fe30Al10 bulk metallic glass. The melting characteristics of Nd61Fe30Zn9 alloy show that its compositional is at a eutectic point, but the alloys exhibit non--eutectic microstructure due to high tendency of undercooled ability.
|
|
Received: 05 June 2003
|
|
|
[1] Chen H S. Acta Metall, 1974; 22:1505 [2] Inoue A, Nishiyama N, Matsuda T. Mater Trans JIM, 1996; 37:181 [3] Schwarz. R B, He Y. Mater Sci Forum, 1997; 235-238:231 [4] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1989; 30:965 [5] Inoue A, Ohtera K, Kita K, Masumoto T. Jpn J appl Phys, 1988; 27:L2248 [6] Inoue A, Zhang T, Masumoto T. Mater Trans JIM, 1990; 31:177 [7] Peker A, Johnson W L. Appl Phys Left, 1993; 63:2342 [8] Inoue A, Shibata, T. Zhang T. Mater Trans JIM, 1995; 36:1420 [9] He Y, Price C, J Pooh S. Philos Mag Let, 1994; 70:371 [10] Zhang T, Inoue A. Mater Trans JIM, 1998; 39:1001 [11] Zhang T, Inoue A. Mater Trans JIM, 1999; 40:301 [12] Inoue A, Zhang T, Zhang W, Takeuchi A. Mater Trans JIM, 1996; 37:99 [13] Inoue A, Zhang T, Takeuchi A, Zhang W. Mater Trans JIM, 1996; 37:636 [14] Inoue A, Takeuchi A, Zhang T. Metall Trans, 1998; A29: 1779 [15] Busch R. JOM, 2002; 52:39 [16] Chen W, Wang Y, Qing J, Dong C. Acta Metall, 2003; 51:1899 [17] Lu Z P, Li Y, Ng S C. J Non-Cryst Solids, 2000; 270:103 [18] Qiu K Q, Zhang Q S, Wang A M, Zhang H F, Ding B Z, Hu Z Q. Acta Metall Sin, 2001; 37:829(邱克强,张庆生,王爱民,张海峰,丁炳哲,胡壮麒.金属学报,2001;37:829) [19] Qiu K Q, Zhang H F, Wang, A M, Ding B Z, Hu Z Q. Acta Metall, 2002; 50:3567 [20] Lu Z P, Li Y, Ng S C, Feng Y P. In: Johnson W L, Inoue A, Liu C T eds, Bulk Metallic Glasses, Pittsburgh, PA: Material Research Society, 1999:205 [21] Guo F Q, Enouf S, Shiflet G, Pooh J. Mater Trans JIM, 2000; 41:1406 [22] Turnbull D M. Contempt Phys, 1969; 10:473 [23] Li Y. Mater Trans JIM, 2001; 42:556 [24] Qiu K Q, Zhang H F, Wang A M, Ding B Z, Hu Z Q. Mater Left (in submitted) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|