| Transformation Kinetics of Undercooled Austenite During Deformation of Low Carbon Mn Steels with Different Carbon and Manganese Contents |
| ZHOU Rongfeng; YANG Wangyue; SUN Zuqing |
| School of Materials Science and Engineering; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
ZHOU Rongfeng; YANG Wangyue; SUN Zuqing. Transformation Kinetics of Undercooled Austenite During Deformation of Low Carbon Mn Steels with Different Carbon and Manganese Contents. Acta Metall Sin, 2004, 40(10): 1055-1063 .
|
|
|
Abstract The effects of carbon and manganese on the kinetics and the ferrite
nucleation of deformation enhanced ferrite
transformation DEFT in low carbon Mn steels were investigated.
It was found that the addition of carbon prolongs the transformation incubation period dramatically, which retards the ransformation kinetics. However, the ransformationincubation
period is somewhat prolonged, and the kinetics becomes much more
sluggish as the manganese content increased. The more
pronounced refinement is achieved as the carbon or manganese content
increased because of the higher nucleation rate, especially in
the steels with high carbon content. The process of DEFT in the tested
steels can be divided into three stages according to the
characteristics of the DEFT kinetics, the first stage obeys Cahn
site saturation mechanism, but the other two stages not.
|
|
Received: 13 November 2003
|
|
|
[1] Sun Z Q, Yang W Y, Qi J J, Hu A M. Mater Sci Eng A,2002; 334: 201 [2] Qi J J, Yang W Y, Sun Z Q. J Univ Sci Technol Beijing,2002; 24(2) : 97(齐俊杰,杨王玥,孙祖庆.北京科技大学学报,2002;24(2) :97) [3] Yang W Y, Hu A M, Qi J J, Sun Z Q. Chin J Mater Res, 2001; 15: 171(杨王玥,胡安民,齐俊杰,孙祖庆.材料研究学报,2001;15:171) [4] Hu A M. Master Thesis, University of Science and Technology Beijing, 2000(胡安民.北京科技大学硕士学位论文.2000) [5] Qi J J. PhD Thesis, University of Science and Technology Beijing, 2002 (齐俊杰.北京科技大学博士学位论文.2002) [6] Zhou R F, Yang W Y, Sun Z Q. Acta Metall Sin, in accepted.(周荣锋,杨王玥,孙祖庆.金属学报,已接受) [7] Zhou R F, Yang W Y, Sun Z Q. Iron Steel, in accepted.(周荣锋,杨王玥,孙祖庆.钢铁,已接受) [8] Yang P, Fu Y Y, Cui F E, Sun Z Q. Acta Metall Sin, 2001; 36: 617(杨平,傅云义,崔风娥,孙祖庆.金属学报,2001;37:617) [9] Kamat R G, Hawbolt E B, Brown L C, Brimacombe J K.Met Trans A, 1992; 23A: 2469 [10] Leslie W C, Rauch G C. Met Trans A, 1978; 9A: 343 [11] Khlestov V M, Konopleva E V, Mcqueen H J. Can MetallQ, 1998; 26(1) : 64 [12] Hickson M R, Hurley P J, Gibbs R K, Kelly G L, HodgsonP. D. Metall Mater Trans A, 2002; 33A: 1019 [13] Cahn J W. Acta Metall, 1956; 9: 449 [14] Hickson M R, Gibbs R K, Hodgson P D. ISIJ Int, 1999;39: 1176V |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|